Magnetic Microstructures of Perpendicular Magnetic-Recording Media

Published online by Cambridge University Press:  29 November 2013

Get access

Extract

Magnetic recording has been the dominant recording technology for information storage since the invention of the computer. Currently, 1-Gbit/in. longitudinal magnetic recording (LMR) systems have been realized and densities of 10 Gbit/in., having bit areas less than 0.1 μm, are being developed. To reach this goal, a drastic scaling down of the track pitch, bit-cell length, head gap, medium thickness, and head-medium spacing is required. If this trend of increasing densities continues, an areal density of more than 300 Gbit/in. is predicted in the 21st century, based on computer simulation using the perpendicular magnetic recording (PMR) mode instead of the current LMR scheme. Magnetic-recording technologies and related materials have already been discussed in another issue of the MRS Bulletin, and hence in this paper, we concentrate on Co-Cr-X material used as a medium for PMR.

The PMR mode has been studied since 1975 and at present, Co-Cr-X (e.g., X = Ta) films with perpendicular anisotropy are the most promising media material. In general, such media should have the following properties: easy axis of magnetization perpendicular to the film plane, suitable coercivity (Hc) and remanent magnetization (Mr) for storing the information and reading it at a high signal-to-noise (S/N) level, uniform columnar size with a small diameter, magnetically uncoupled columns having a magnetization reversal based on rotation instead of a domain-wall motion, chemical stability under various environmental conditions, and a small surface roughness. In order to achieve the desired magnetic anisotropy and coercivity, a columnar morphology (small diameter) with an hep [0001] texture and exchange-decoupled, columnar boundaries—to create a magnetic microstructure for single domain switching columns with high coercivity—should be obtained. An overview of the preparation, microstructure, and magnetic properties of Co-Cr thin films is given in Reference 8. Depending on the deposition parameters, a so-called initial layer (with an in-plane magnetization) can be present.

Type
Magnetism on a Microscopic Scale
Copyright
Copyright © Materials Research Society 1995

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

1.Yogi, T., Tsang, C., Nguyen, T.A., Ju, K., Gorman, G.L., and Castillo, G., IEEE Trans. Magn. 26 (5) (1990) p. 2271.CrossRefGoogle Scholar
2.Futamoto, M., Kugiya, F., Suzuki, M., Takano, H., Matsuda, Y., Inabe, N., Miyamura, Y., Akagi, K., Nakano, T., and Sawaguchi, H., IEEE Trans. Magn. 27 (1991) p. 5280.CrossRefGoogle Scholar
3.Murdock, E.S., Simmons, R.F., and Davidson, R., IEEE Trans. Magn. 28 (1992) p. 3078.CrossRefGoogle Scholar
4.Nakamura, Y., J. Magn. Soc. Jpn. 15 (S2) (1991) p. 497.CrossRefGoogle Scholar
5.Tagawa, I. and Nakamura, Y., IEEE Trans. Magn. 13 (S1) (1989) p. 97.Google Scholar
6. See the various contributions in “Magnetic Recording Materials,” MRS Bulletin XV (3) (1990) p. 23.Google Scholar
7.Iwasaki, S. and Takemura, K., IEEE Trans. Magn. 11 (1975) p. 1173.CrossRefGoogle Scholar
8.Lodder, J.C., “Preparation, Microstructure and Magnetic Properties of Co-Cr Thin Films,” Chapter 6, p. 161; in High Density Recording, edited by K.H.J. Buschow, G.J. Long, and F. Grandjean (Kluwer Academic Publishers, NATO ASI Applied Sciences, Vol. 229, 1993).Google Scholar
9.Maeda, Y., Hirono, S., and Asahi, M., Jpn. J. Appl. Phys. 24 (1985) p. L951.CrossRefGoogle Scholar
10.Hono, K., Babu, S.S., Maeda, Y., Hasegawa, N., and Sakurai, T., Appl. Phys. Lett. 62 (1993) p. 2504.CrossRefGoogle Scholar
11.de Haan, S., Lodder, J.C., and Popma, A.J., J. Magn. Soc. Jpn. 15 (S2) (1991) p. 349.Google Scholar
12.Ruhrig, M., Porthun, S., and Lodder, J.C., Rev. Sci. Instrum. 63 (10) (1994) p. 3224.CrossRefGoogle Scholar
13.van Kooten, M., de Haan, S., Lodder, J.C., and Popma, A.J., J. Appl. Phys. 75 (10) (1994) p. 5508.CrossRefGoogle Scholar
14.Lodder, J.C., Wielinga, T., and Worst, J., Thin Solid Films 101 (1982) p. 61.CrossRefGoogle Scholar
15.Brown, W.F. Jr., Rev. Mod. Phys. 17 (1945) p. 15.CrossRefGoogle Scholar
16.den Boef, A., Appl. Phys. Lett. 55 (1989) p. 439.CrossRefGoogle Scholar
17.Nakamura, Y., Muraoka, H., Watanabe, I., and Inaguma, T., J. Magn. Soc. Jpn. 18 (S1) (1994) p. 583.CrossRefGoogle Scholar