High speed edge cracks and holes detection at the exit of theBasse-Indre tandem cold mill

Published online by Cambridge University Press:  29 November 2006

Get access

Abstract

An automatic detection system for edge cracks and holes has beensuccessfully installed at the exit of the tin plate mill of the API Basse-Indre plant. This new system is able to detect, analyze and recordimages of any defect that may be dangerous for the CAL. Since thesystem has been implemented, Basse-Indre has recorded no breakageneither in the furnace along year 2005, nor at entry, at exit or inthe furnace since early 2006.