Article contents
Duplex and Superduplex stainless steel grades for wet fluegas desulphurisation systems
Published online by Cambridge University Press: 05 June 2008
Abstract
The corrosion risks in a wet flue gas desulphurization systemenvironment are reported. Uniform and localized corrosionresistance of different stainless steels is studied by electrochemicaltests. The effects of chloride content, fluoride content, pH andtemperature on corrosion resistance are discussed. The results showthat duplex UNS S32205 or superduplex UNS S32520 gradesare prime substitutes for austenitic 317LNM or super austenitic likeUNS S34565 grades in many aggressive environments. The lifecycle costs of scrubbers constructed of stainless steels plates or cladplates are compared. The excellent corrosion resistance of duplexand superduplex stainless steels, combined with their increasedmechanical properties and moderate alloy cost afford very costeffective solutions for wet flue gas desulphurization.
- Type
- Research Article
- Information
- Metallurgical Research & Technology , Volume 105 , Issue 5: Coke plantSinteringSteelmakingHot RollingSteel Use , May 2008 , pp. 286 - 295
- Copyright
- © La Revue de Métallurgie, 2008
- 2
- Cited by