Hostname: page-component-586b7cd67f-t7czq Total loading time: 0 Render date: 2024-11-27T03:34:15.935Z Has data issue: false hasContentIssue false

Wear resistance of arc ion-plated chromium nitride coatings

Published online by Cambridge University Press:  31 January 2011

Yuji Chiba
Affiliation:
Central Research Laboratory, Sumitomo Metal Mining Co. Ltd., 18-5, 3-chome, Nakakokubun Ichikawa 272, Japan
Toshio Omura
Affiliation:
Central Research Laboratory, Sumitomo Metal Mining Co. Ltd., 18-5, 3-chome, Nakakokubun Ichikawa 272, Japan
Hiroshi Ichimura
Affiliation:
Central Research Laboratory, Sumitomo Metal Mining Co. Ltd., 18-5, 3-chome, Nakakokubun Ichikawa 272, Japan
Get access

Abstract

Wear resistance of arc ion-plated chromium nitride films has been studied. It has been found that texture and phases composing the films depend much on bias voltage and nitrogen gas pressure at the deposition. A phase diagram was constructed as a function of these two parameters, which indicated that three categories exist: CrN single, CrN and Cr2N dual, and CrN and Cr dual phased regions, respectively. Results of Falex No. 2 test showed that the wear resistance of CrN single phased films is superior to others, especially when (220) preferred orientation is developed. Since hardness and surface morphology do not differ much between these films, a high toughness of CrN single phased film is considered to make a difference by suppressing abrasion wear.

Type
Articles
Copyright
Copyright © Materials Research Society 1993

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

REFERENCES

1Komiya, S.Ono, S.Umezu, N. and Narusawa, T.Thin Solid Films 45, 433 (1977).Google Scholar
2Aubert, A.Gillet, R.Gaudier, A. and Terrat, J.P.Thin Solid Films 108, 165 (1983).CrossRefGoogle Scholar
3Kawana, A. and Ichimura, H. in High Temperature Corrosion of Advanced Materials and Protective Coating, edited by Saito, Y.Oney, B. and Maruyama, T. (Elsevier Science Publishers, Amsterdam, 1992), p. 267.CrossRefGoogle Scholar
4Kashiwagi, K.Kobayashi, K.Masuyama, A. and Murayama, Y.J. Vac. Sci. Technol. A4, 210 (1986).Google Scholar
5Wang, D. and Oki, T.Thin Solid Films 185, 219 (1990).CrossRefGoogle Scholar
6Bergman, C. in Ion Plating and Implantation, edited by Hochman, R. F. (American Society for Metals, Metals Park, OH, 1986), p. 115.Google Scholar
7Steinmann, P. A. and Hintermann, H. E.J. Vac. Sci. Technol. A3, 2349 (1985).Google Scholar
8Hollock, H.J. Vac. Sci. Technol. A4, 2661 (1986).Google Scholar
9Petch, N.J.Prog. Met. Phys. 5, 1 (1954).CrossRefGoogle Scholar
10Yamamoto, S. and Ichimura, H.J. Mater. Res. 7, 2240 (1992).Google Scholar
11Niihara, K.Bull. Ceram. Soc. Jpn. 20, 12 (1985).Google Scholar