Hostname: page-component-cd9895bd7-gxg78 Total loading time: 0 Render date: 2024-12-23T12:28:40.956Z Has data issue: false hasContentIssue false

The Spreading Kinetics of Ag–28Cu(L) on Nickel(S): Part II. Area of Spread on Surfaces Plated with Electrolytic Ni

Published online by Cambridge University Press:  31 January 2011

Douglas A. Weirauch Jr
Affiliation:
Ceramics Technology Center, Alcoa Technical Center, Alcoa Center, Pennsylvania 15069
Stephen F. Horvath
Affiliation:
Alcoa Electronic Packaging, San Diego, California
Get access

Abstract

Furnace brazing is commonly used in the electronic industry to attach I/O pins, lid-seal rings, and heat spreaders to cofired multilayer ceramic packages. Despite the widespread industry usage of electrolytic and electroless Ni coatings to render base metal surfaces wettable by braze fillers, there is no fundamental treatment of “brazeability” in the published literature that can be used by the materials technologist to design coatings for a given application. In this study, dynamic hot stage microscopy is used to establish the parameters that control the spreading of eutectic Ag–Cu braze on surfaces plated with electrolytic Ni. The effects of plating thickness, substrate type, plating annealing, and the braze thermal cycle are considered. A braze spreading mechanism developed for polycrystalline Ni foil in Part I of this study is linked to Ni-plated surfaces through consideration of differences in microstructure. Eventual extension of this improved understanding to surfaces plated with electroless Ni–B and Ni–P deposits will result in shortened product design time and improved manufacturing process control.

Type
Articles
Copyright
Copyright © Materials Research Society 1997

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

1.Sahara, H., Emoto, Y., and Otsuka, K., in Proc. 32nd IEEE Elec. Components Conf. (1982), p. 32.Google Scholar
2.Weirauch, D. A., Jr., Welding J. 73, 110s (1994).Google Scholar
3.Williams, J. C. and Neilsen, J. W., J. Am. Ceram. Soc. 42, 229 (1959).CrossRefGoogle Scholar
4.Hey, A. W., in Joining of Ceramics, edited by Nicholas, M. G. (Chapman and Hall, London, 1990), p. 56.Google Scholar
5.Keusseyan, R. L., Goeller, P. T., Page, J. P., Osborne, J. J., Nebe, W. J., and Polzer, E. K., in Proc. IEEE/ISHM ‘90 IEMT Symp., Italy(1990), p. 186.Google Scholar
6.Humpston, G. and Jacobson, D. M., in Principles of Soldering and Brazing (ASM INTERNATIONAL, Materials Park, OH, 1993), p. 188.Google Scholar
7.Weirauch, D. A., Jr. and Krafick, W. J., J. Mater. Res. 11, 1897 (1996).CrossRefGoogle Scholar
8.Kim, H. K., Liou, H. K., and Tu, K. N., J. Mater. Res. 10, 497 (1995).CrossRefGoogle Scholar
9.Chen, S-W., Mater. Chem. Phys. 33, 271 (1993).Google Scholar
10.Jacobson, B. E. and Silwa, J. W., Plating and Surface Finishing 66 (9), 42 (1979).Google Scholar
11.Lawless, K. R., in Physics of Thin Films, edited by Hass, G. and Thun, R. E. (Academic Press, New York, 1967), Vol. 4, p. 191.Google Scholar
12.Weil, R., 1974, Plating, July, 654 (1974).Google Scholar
13.Schwartz, M., in Deposition Technologies for Films and Coatings, Developments and Applications, edited by Bunshah, R. F. (Noyes Publications, Park Ridge, NJ, 1982), p. 385.Google Scholar