Crossref Citations
This article has been cited by the following publications. This list is generated based on data provided by
Crossref.
Liau, Leo Chau-Kuang
and
Tung, Ming-Te
2006.
Kinetic Investigation of Photocatalytic Effects on Poly(vinyl butyral) Photodegradation.
Industrial & Engineering Chemistry Research,
Vol. 45,
Issue. 7,
p.
2199.
Lombardo, Stephen J.
Yun, Jeong Woo
and
Krueger, Daniel S.
2006.
Innovative Processing and Synthesis of Ceramics, Glasses and Composites VIII.
Vol. 166,
Issue. ,
p.
191.
Yun, Jeong Woo
and
Lombardo, Stephen J.
2006.
Heat Transfer in Porous Green Bodies During Binder Removal by Minimum Time Heating Cycles.
Journal of the American Ceramic Society,
Vol. 89,
Issue. 4,
p.
1193.
Yun, Jeong Woo
Lombardo, Stephen J.
Krueger, Daniel S.
and
Scheuer, Peter
2006.
Effect of Decomposition Kinetics and Failure Criteria on Binder‐Removal Cycles From Three‐Dimensional Porous Green Bodies.
Journal of the American Ceramic Society,
Vol. 89,
Issue. 1,
p.
176.
Lombardo, S. J.
Yun, J. W.
Krueger, D. S.
and
Scheuer, P. J.
2006.
Advances in Dielectric Materials and Electronic Devices.
Vol. 174,
Issue. ,
p.
305.
Liau, Leo Chau‐Kuang
and
Chien, Yu‐Ching
2006.
Kinetic investigation of ZrO2, Y2O3, and Ni on poly(vinyl butyral) thermal degradation using nonlinear heating functions.
Journal of Applied Polymer Science,
Vol. 102,
Issue. 3,
p.
2552.
Feng, Z. C.
Ha, S. W.
Lombardo, S. J.
Yun, J. W.
Krueger, D. S.
and
Scheuer, P. J.
2006.
Innovative Processing and Synthesis of Ceramics, Glasses and Composites IX.
Vol. 177,
Issue. ,
p.
81.
Yun, Jeong Woo
and
Lombardo, Stephen J.
2007.
Permeability of Green Ceramic Tapes as a Function of Binder Loading.
Journal of the American Ceramic Society,
Vol. 90,
Issue. 2,
p.
456.
Yun, Jeong Woo
and
Lombardo, Stephen J.
2008.
Permeability of Laminated Green Ceramic Tapes as a Function of Binder Loading.
Journal of the American Ceramic Society,
Vol. 91,
Issue. 5,
p.
1553.
Yun, Jeong Woo
and
Lombardo, Stephen J.
2008.
Scaling Analysis of the Effect of Binder Content and Binder Distribution on the Gas Permeability of Porous Green Ceramics.
Journal of the American Ceramic Society,
Vol. 91,
Issue. 7,
p.
2150.
Liau, Leo Chau-Kuang
and
Chen, Chung-Chun
2008.
Optimal heating trajectories of controlling green tapes of YSZ electrolyte deformation using TMA during thermal processing.
Journal of Power Sources,
Vol. 177,
Issue. 1,
p.
1.
Yun, J. W.
and
Lombardo, S. J.
2009.
Determination of rapid heating cycles for binder removal from open pore green ceramic components.
Advances in Applied Ceramics,
Vol. 108,
Issue. 2,
p.
92.
Lombardo, S. J.
Yun, J.W.
and
Patel, S.
2009.
Advances in Electroceramic Materials.
p.
89.
Mohsin, Ijaz Ul
Gierl, Christian
Danninger, Herbert
and
Momeni, Mohammad
2011.
Thermal de-binding kinetics of injection molded W-8%Ni-2%Cu.
International Journal of Refractory Metals and Hard Materials,
Vol. 29,
Issue. 6,
p.
729.
Lombardo, Stephen J.
and
Franks, G.
2013.
Analytic Model for the Diffusant Concentration in Ceramic Green Bodies During Diffusion‐Controlled Thermal Binder Removal.
Journal of the American Ceramic Society,
Vol. 96,
Issue. 9,
p.
2737.
Lee, Seung Jin
Lee, Jeong Myeong
Kim, Yoon Gon
Yoon, Soon Do
and
Yun, Jeong Woo
2014.
Thermal cycle development of PMMA pore former removal for honeycomb-type SOFC supports.
Ceramics International,
Vol. 40,
Issue. 3,
p.
4879.
Lombardo, Stephen J.
and
Suvaci, E.
2015.
Minimum Time Heating Cycles for Diffusion‐Controlled Binder Removal from Ceramic Green Bodies.
Journal of the American Ceramic Society,
Vol. 98,
Issue. 1,
p.
57.
Lombardo, Stephen J.
2017.
Minimum time heating cycles for diffusion‐ versus permeability‐controlled binder removal from ceramic green bodies.
Journal of the American Ceramic Society,
Vol. 100,
Issue. 2,
p.
529.
Hedayat, Nader
Du, Yanhai
and
Ilkhani, Hoda
2018.
Pyrolyzable pore-formers for the porous-electrode formation in solid oxide fuel cells: A review.
Ceramics International,
Vol. 44,
Issue. 5,
p.
4561.
Lombardo, Stephen J.
and
Retzloff, David G.
2019.
A process control algorithm for reaction‐diffusion minimum time heating cycles for binder removal from green bodies.
Journal of the American Ceramic Society,
Vol. 102,
Issue. 3,
p.
1030.