Preparation of barium hexa-aluminate aerogel

Published online by Cambridge University Press:  03 March 2011

Yasuyuki Mizushima
Affiliation:
Colloid Research Institute, 350-1 Ogura, Yahatahigashi-ku, Kitakyushu 805, Japan
Makoto Hori
Affiliation:
Colloid Research Institute, 350-1 Ogura, Yahatahigashi-ku, Kitakyushu 805, Japan
Get access

Abstract

Barium hexa-aluminate (BaO · 6Al2O3) aerogels were prepared using a supercritical drying method and their properties examined. A barium hexa-aluminate aerogel prepared from a double alkoxide of barium and aluminum showed a high specific surface area of 421 m2/g. Monolithic barium hexa-aluminate formed. No BaO · Al2O3 or alumina was observed, as is often the case in powder processing. The specific surface area of the monolithic barium hexa-aluminate fired at 1400 °C for 2 h was 12 m2/g, while that of the barium hexa-aluminate xerogel was only 0.8 m2/g. A barium hexa-aluminate aerogel was also prepared using barium by using a chelating agent. This aerogel showed a specific surface area of 454 m2/g as-dried. In the case of the chelating agent, BaO · Al2O3 was also detected along with barium hexa-aluminate after firing.

Type
Articles
Copyright
Copyright © Materials Research Society 1994

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

REFERENCES

1Ichikawa, T., Kakuta, N., and Ueno, A., Proceedings of the First Tokyo Conference on Advanced Catalytic Science and Technology, Tokyo (1990), p. 521.Google Scholar
2Arai, H., Yamada, T., Eguchi, K., and Seiyama, T., Appl. Catal. 26, 265 (1986).CrossRefGoogle Scholar
3Maeda, K., Mizukami, F., Watanabe, M., Arai, N., Toba, M., and Shimizu, K., J. Mater. Sci. Lett. 9, 522 (1990).CrossRefGoogle Scholar
4Young, D. J., Udaja, P., and Trimm, D. L., in Catalyst Deactivation (Elsevier, New York, 1980), p. 331.CrossRefGoogle Scholar
5Burggraaf, A. J., Keiser, K., and van Hassel, B. A., Solid State Ionics 32/33, 771 (1989).CrossRefGoogle Scholar
6Amato, I., Martoma, D., and Silengo, B., in Sintering and Catalysis, edited by Kuczynski, G. C. (Plenum Press, New York/London, 1975), p. 187.CrossRefGoogle Scholar
7Machida, M., Eguchi, K., and Arai, H., Chem. Lett., 1993 (1986).CrossRefGoogle Scholar
8Machida, M., Eguchi, K., and Arai, H., J. Catal. 103, 385 (1987).CrossRefGoogle Scholar
9Mizushima, Y. and Hori, M., J. Mater. Res. 8, 2993 (1993).CrossRefGoogle Scholar
10Burggraaf, A. J., Keiser, K., and van Hassel, B. A., Surf. Interf. Ceram. Mater. 705 (1989).Google Scholar
11Bradley, D. C., Mehrotra, R. C., and Gaur, D. P., Metal Alkoxides (Academic Press, London, 1978), p. 306.Google Scholar
12Japan Patent No. 62-322846.Google Scholar
13Babonneau, F., Coury, L., and Livage, J., J. Non-Cryst. Solids 121, 153157 (1990).CrossRefGoogle Scholar
14Machida, M., Eguchi, K., and Arai, H., J. Am. Ceram. Soc. 71, 1142 (1988).CrossRefGoogle Scholar