Hostname: page-component-586b7cd67f-dsjbd Total loading time: 0 Render date: 2024-11-26T09:02:53.472Z Has data issue: false hasContentIssue false

Hydrogen embrittlement behaviors of ultrafine-grained 22Mn–0.6C austenitic twinning induced plasticity steel

Published online by Cambridge University Press:  20 September 2017

Yu Bai*
Affiliation:
Department of Materials Science and Engineering, Kyoto University, Kyoto 606-8501, Japan; and Elements Strategy Initiative for Structural Materials (ESISM), Kyoto University, Kyoto 606-8501, Japan
Yanzhong Tian
Affiliation:
Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, People’s Republic of China
Si Gao
Affiliation:
Department of Materials Science and Engineering, Kyoto University, Kyoto 606-8501, Japan
Akinobu Shibata
Affiliation:
Department of Materials Science and Engineering, Kyoto University, Kyoto 606-8501, Japan; and Elements Strategy Initiative for Structural Materials (ESISM), Kyoto University, Kyoto 606-8501, Japan
Nobuhiro Tsuji*
Affiliation:
Department of Materials Science and Engineering, Kyoto University, Kyoto 606-8501, Japan; and Elements Strategy Initiative for Structural Materials (ESISM), Kyoto University, Kyoto 606-8501, Japan
*
a)Address all correspondence to this author. e-mail: [email protected]
Get access

Abstract

Hydrogen embrittlement behaviors of a 22Mn–0.6C (mass%) twinning induced plasticity (TWIP) steel with the grain sizes of 21 μm (coarse grain) and 0.58 μm (ultrafine grain) were investigated by means of hydrogen precharging and subsequent slow strain rate tensile tests. The total elongation and fracture stress for both of the coarse-grained and ultrafine-grained specimens decreased by hydrogen charging. The area fraction of the brittle fracture surfaces in the ultrafine-grained specimen was much smaller than that in the coarse-grained specimen. Three-point bending test also showed that the reduction of the fracture toughness by the introduction of hydrogen was much smaller in the ultrafine-grained specimen than that in the coarse-grained specimen. It was concluded that the suppressed hydrogen embrittlement by grain refinement in the 22Mn–0.6C TWIP steel was probably due to the smaller hydrogen contents per unit grain boundary area in the finer grain-sized material.

Type
Articles
Copyright
Copyright © Materials Research Society 2017 

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Footnotes

Contributing Editor: Mathias Göken

References

REFERENCES

Grassel, O. and Frommeyer, G.: Effect of martensitic phase transformation and deformation twinning on mechanical properties of Fe–Mn–Si–Al steels. Mater. Sci. Technol. 14, 1213 (1998).CrossRefGoogle Scholar
Ueji, R., Tsuchida, N., Terada, D., Tsuji, N., Tanaka, Y., Takamura, A., and Kunishige, K.: Tensile properties and twinning behavior of high manganese austenitic steel with fine-grained structure. Scr. Mater. 59, 963 (2008).Google Scholar
Bouaziz, O., Allian, S., Scott, C.P., Cugy, P., and Barbier, D.: High manganese austenitic twinning induced plasticity steels: A review of the microstructure properties relationships. Curr. Opin. Solid State Mater. Sci. 15, 141 (2011).Google Scholar
Adler, P.H., Olson, G.B., and Owen, W.S.: Strain hardening of Hadfield manganese steel. Metall. Mater. Trans. A 17, 1725 (1986).Google Scholar
Cooman, B.C.D., Kwon, O., Chin, K.G.: State-of-the-knowledge on TWIP steel. Mater. Sci. and Tech. 28, 513 (2012).Google Scholar
Frommeyer, G., Brux, U., and Neumann, P.: Supra-ductile and high-strength manganese–TRIP/TWIP steels for high energy absorption purposes. ISIJ Int. 43, 438 (2003).CrossRefGoogle Scholar
Koyama, M., Akiyama, E., and Tsuzaki, K.: Effect of hydrogen content on the embrittlement in a Fe–Mn–C twinning-induced plasticity steel. Corros. Sci. 59, 277 (2012).Google Scholar
Park, I.J., Jeong, K.H., Jung, J.G., Lee, C.S., and Lee, Y.K.: The mechanism of enhanced resistance to the hydrogen delayed fracture in Al-added Fe–18Mn–0.6C twinning-induced plasticity steels. Int. J. Hydrogen Energy 37, 9925 (2012).CrossRefGoogle Scholar
Koyama, M., Akiyama, E., Tsuzaki, K., and Raabe, D.: Hydrogen-assisted failure in a twinning-induced plasticity steel studied under in situ hydrogen charging by electron channeling contrast imaging. Acta Mater. 61, 4607 (2013).CrossRefGoogle Scholar
Koyama, M., Akiyama, E., Sawaguchi, T., Raabe, D., and Tsuzaki, K.: Hydrogen-induced cracking at grain and twin boundaries in an Fe–Mn–C austenitic steel. Scr. Mater. 66, 459 (2012).Google Scholar
Koyama, M., Akiyama, E., and Tsuzaki, K.: Hydrogen embrittlement in a Fe–Mn–C ternary twinning-induced plasticity steel. Corros. Sci. 54, 1 (2012).Google Scholar
Ryu, J.H., Kim, S.K., Lee, C.S., Suh, D.W., and Bhadeshia, H.K.D.H.: Effect of aluminum on hydrogen-induced fracture behavior in austenitic Fe–Mn–C steel. Proc. R. Soc., Ser. A 469, 20120458 (2012).CrossRefGoogle Scholar
Chin, K.G., Kang, C.Y., Shin, S.Y., Hong, S., Lee, S., Kim, H.S., Kim, K.H., and Kim, N.J.: Effects of Al addition on deformation and fracture mechanisms in two high manganese TWIP steels. Mater. Sci. Eng., A 528, 2922 (2011).CrossRefGoogle Scholar
Shibata, A., Takahashi, H., and Tsuji, N.: Microstructural and crystallographic features of hydrogen-related crack propagation in low carbon martensitic steel. ISIJ Int. 52, 208 (2012).Google Scholar
Park, I.J., Lee, S.M., Jeon, H.H., and Lee, Y.K.: The advantage of grain refinement in the hydrogen embrittlement of Fe–18Mn–0.6C twinning-induced plasticity steel. Corros. Sci. 93, 63 (2015).Google Scholar
Zan, N., Ding, H., Guo, X.F., Tang, Z.Y., and Bleck, W.: Effects of grain size on hydrogen embrittlement in a Fe–22Mn–0.6C TWIP steel. Int. J. Hydrogen Energy 40, 10687 (2015).Google Scholar
Michler, T., Marchi, C.S., Naumann, J., Weber, S., and Martin, M.: Hydrogen environment embrittlement of stable austenitic steels. Int. J. Hydrogen Energy 37, 16231 (2012).Google Scholar
Chen, S.H., Zhao, M.J., and Rong, L.J.: Effect of grain size on the hydrogen embrittlement sensitivity of a precipitation strengthened Fe–Ni based alloy. Mater. Sci. Eng., A 594, 98 (2014).CrossRefGoogle Scholar
Saha, R., Ueji, R., and Tsuji, N.: Fully recrystallized nanostructure fabricated without severe plastic deformation in high-Mn austenitic steel. Scr. Mater. 68, 813 (2013).Google Scholar
Bai, Y., Momotani, Y., Chen, M.C., Shibata, A., and Tsuji, N.: Effect of grain refinement on hydrogen embrittlement behaviors of high-Mn TWIP steel. Mater. Sci. Eng., A 651, 935 (2016).Google Scholar
Tian, Y.Z., Bai, Y., Chen, M.C., Shibata, A., Terada, D., and Tsuji, N.: Enhanced strength and ductility in an ultrafine-grained Fe–22Mn–0.6C austenitic steel having fully recrystallized structure. Metall. Mater. Trans. A 45, 5300 (2014).Google Scholar
Dumay, A., Chateau, J.P., Allain, S., Migot, S., and Bouaziz, O.: Influence of addition elements on the stacking-fault energy and mechanical properties of an austenitic Fe–Mn–C steel. Mater. Sci. Eng., A 483–484, 184 (2008).Google Scholar
Nagumo, M., Takai, K., and Okuda, N.: Nature of hydrogen trapping sites in steels induced by plastic deformation. J. Alloys Compd. 293–295, 310 (1999).Google Scholar
Choo, W.Y. and Lee, J.Y.: Thermal analysis of trapped hydrogen in pure iron. Metall. Mater. Trans. A 13, 135 (1982).Google Scholar
Tsuchida, T., Hara, T., and Tsuzaki, K.: Relationship between microstructure and hydrogen absorption behavior in a V-bearing high strength steel. Tetsu to Hagane 88, 771 (2002).CrossRefGoogle Scholar
Takai, K. and Watanuki, R.: Hydrogen in trapping states innocuous to environmental degradation of high-strength steels. ISIJ Int. 43, 520 (2003).Google Scholar
Chêne, J., Aucouturier, M., Arnould-Laurent, R., Tison, P., and Fidelle, J.P.: Hydrogen transport by dislocations and hydrogen embrittlement in stainless steels. In Third International Conference on the Effect of Hydrogen on Behavior of Materials, Bernstein, I.M. and Thompson, A.W., eds. (Jackson Lake, Wyoming, USA, 1981); p. 583.Google Scholar
Chun, Y.S., Park, K.T., and Lee, C.S.: Delayed static failure of twinning-induced plasticity steels. Scr. Mater. 66, 960 (2012).Google Scholar
Ronevich, J.A., Kim, S.K., Speer, J.G., and Matlock, D.K.: Hydrogen effects on cathodically charged twinning-induced plasticity steel. Scr. Mater. 66, 956 (2012).CrossRefGoogle Scholar
Tsuji, N., Ito, Y., Sato, Y., and Miyamoto, Y.: Strength and ductility of ultrafine grained aluminum and iron produced by ARB and annealing. Scr. Mater. 47, 893 (2002).Google Scholar
Michler, T., Marchi, C.S., Naumann, J., Weber, S., Martin, M.: Hydrogen environment embrittlement of stable austenitic steels. Inter. J. Hydrogen Energy 37, 16231 (2012).Google Scholar
So, K.H., Kim, J.S., Chun, Y.S., Park, K.T., Lee, Y.K., and Lee, C.S.: Hydrogen delayed fracture properties and internal hydrogen behavior of a Fe–18Mn–1.5Al–0.6C TWIP steel. ISIJ Int. 49, 1952 (2009).Google Scholar
Oriani, R.A., Hirth, J.P., and Smialowski, M.: Hydrogen Degradation of Ferrous Alloy (Noyes Publications, Park Ridge, 1985).Google Scholar
Weertman, J. and Weertman, J.R.: Elementary Dislocation Theory (Oxford University Press, New York, 1992).Google Scholar