Effect of heat treatment on formation of sol-gel (Pb, La)TiO3 films for optical application

Published online by Cambridge University Press:  31 January 2011

Junmo Koo
Affiliation:
Department of Materials Science and Engineering, Korea Advanced Institute of Science and Technology (KAIST), Taejon 305-701, Korea
Sung-Uk Kim
Affiliation:
Department of Materials Science and Engineering, Korea Advanced Institute of Science and Technology (KAIST), Taejon 305-701, Korea
Dae Sung Yoon
Affiliation:
Department of Materials Science and Engineering, Korea Advanced Institute of Science and Technology (KAIST), Taejon 305-701, Korea
Kwangsoo No
Affiliation:
Department of Materials Science and Engineering, Korea Advanced Institute of Science and Technology (KAIST), Taejon 305-701, Korea
Byeong-Soo Bae
Affiliation:
Department of Materials Science and Engineering, Korea Advanced Institute of Science and Technology (KAIST), Taejon 305-701, Korea
Get access

Abstract

Lead lanthanum titanate [(Pb, La)TiO3] sol-gel films have been prepared to investigate the effect of heat treatment on the fabrication of uniform and crack-free thick films by applying different heating schedules. The surface morphology as well as the optical properties such as refractive index, optical transmission, and optical propagation loss of the films was examined, depending on the film thickness. Because the slower and longer heating is enough to remove the organic and nitrate residues and diminish the thermal shock while heating the films, slower and longer heating can produce the uniform and crack-free thick films having higher refractive index as well as lower optical propagation loss. Also, the drying and heating of the films on a hot plate in every coating resulted in the fabrication of thick films having above 8000 Å without any defects and microcracks. This film presented the highest refractive index as well as the lowest optical propagation loss which grows exponentially with increasing the film thickness due to the scattering of defects in the film.

Type
Articles
Copyright
Copyright © Materials Research Society 1997

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

1.Haertling, G. H., Integrated Ferroelectrics 3, 207 (1993).CrossRefGoogle Scholar
2.Adachi, H., J. Appl. Phys. 60, 2, 736 (1986).CrossRefGoogle Scholar
3.Teowee, G., Ph.D. Thesis, The University of Arizona, Tucson, AZ (1992).Google Scholar
4.Higashino, H., Kawaguchi, T., Adachi, H., Makino, T., and Yamazaki, O., Jpn. J. Appl. Phys. 24, 2, 284 (1985).CrossRefGoogle Scholar
5.Teowee, G., Boulton, J. M., and Uhlmann, D. R., in Better Ceramics Through Chemistry V, edited by Hampden-Smith, M. J., Klemperer, W. G., and Brinker, C. J. (Mater. Res. Soc. Symp. Proc. 271, Pittsburgh, PA, 1992), p. 345.Google Scholar
6.Vest, R. W. and Xu, J., Ferroelectrics 93, 21 (1989).CrossRefGoogle Scholar
7.Sun, P., Zhang, L., and Yao, X., edited by Liu, M., Safari, A., Kingon, A., and Haertling, G. (8th IEEE Int. Symp. Proc., Ferroelectrics, Greenville, SC, April 1992), p. 432.Google Scholar
8.Teowee, G., Boulton, J. M., Motakef, S., Uhlmann, D. R., Zelinski, B. J. J., Zanoni, R., and Moon, M., SPIE 1758, 236 (1992).Google Scholar
9.Liu, Y., Ren, W., Qiu, J. H., Zhang, L. Y., and Yao, X., Ferroelectrics 152, 195 (1993).CrossRefGoogle Scholar
10.Yoon, D. S., Kim, S. U., Koo, J., Jiang, Z-T., Bae, B-S., Lee, W. J., No, K., and Cho, S. H., Kor. J. Ceram. 1, 4 (1995).Google Scholar
11.Wood, V. E., Busch, J. R., Ramamurthi, S. D., and Swartz, S. L., J. Appl. Phys. 71, 9 (1992).Google Scholar
12.Swanepoel, R., J. Phys. E; Sci. Instrum. 16, 1214 (1983).CrossRefGoogle Scholar
13.Epstein, K. A., Misemer, D. K., and Vernstrom, G. D., Appl. Opt. 26 (2), 294 (1987).CrossRefGoogle Scholar
14.Ulrich, R. and Torge, R., Appl. Opt. 12 (12), 2901 (1973).CrossRefGoogle Scholar
15.Tien, P. K., Ulrich, R., and Matin, R. J., Appl. Phys. Lett. 14 (9), 291 (1969).CrossRefGoogle Scholar
16.Tien, P. K. and Ulrich, R., J. Opt. Soc. Am. 60 (10), 1325 (1970).CrossRefGoogle Scholar
17.Okuyama, M., Usuki, T., Hamakawa, Y., and Nakagawa, T., Appl. Phys. 21, 339 (1980).CrossRefGoogle Scholar
18.Tossell, D. A., Obhi, J. S., Shorrocks, N. M., and Whatmore, R. W. (ISAF IEEE Int. Symp. on the Appl. of Ferroelectrics, Sep. 1992).Google Scholar
19.Fork, D. K., Armani-Leplingard, F., Kingston, J. J., and Anderson, G. B., in Thin Films for Integrated Optics Applications, edited by Wessels, B. W., Marder, S. R., and Walba, D. M. (Mater. Res. Soc. Symp. Proc. 392, Pittsburgh, PA, 1995), p. 189.Google Scholar