Hostname: page-component-586b7cd67f-r5fsc Total loading time: 0 Render date: 2024-11-20T06:43:59.749Z Has data issue: false hasContentIssue false

Dramatically enhanced impact toughness in welded ultra-ferritic stainless steel by additional nitrogen gas in Ar-based shielding gas

Published online by Cambridge University Press:  02 November 2016

Heng Li
Affiliation:
College of Materials Science and Engineering, Taiyuan University of Technology, 030024 Taiyuan, Shanxi Province, China
Wenqing Xing
Affiliation:
College of Materials Science and Engineering, Taiyuan University of Technology, 030024 Taiyuan, Shanxi Province, China
Xinye Yu
Affiliation:
College of Materials Science and Engineering, Taiyuan University of Technology, 030024 Taiyuan, Shanxi Province, China
Wei Zuo
Affiliation:
College of Materials Science and Engineering, Taiyuan University of Technology, 030024 Taiyuan, Shanxi Province, China
Le Ma
Affiliation:
College of Materials Science and Engineering, Taiyuan University of Technology, 030024 Taiyuan, Shanxi Province, China
Peng Dong
Affiliation:
College of Materials Science and Engineering, Taiyuan University of Technology, 030024 Taiyuan, Shanxi Province, China
Wenxian Wang
Affiliation:
College of Materials Science and Engineering, Taiyuan University of Technology, 030024 Taiyuan, Shanxi Province, China; and Key Laboratory of Interface Science and Engineering in Advanced Materials, Ministry of Education, 030024 Taiyuan, Shanxi Province, China
Guangwei Fan
Affiliation:
Key Laboratory of Interface Science and Engineering in Advanced Materials, Ministry of Education, 030024 Taiyuan, Shanxi Province, China; and Technology Center, Taiyuan Iron and Steel (Group) Company Limited, 030003 Taiyuan, China; and Technology Center, Taiyuan Iron and Steel (Group) Company Limited, 030003 Taiyuan, China
Jie Lian
Affiliation:
Key Laboratory of Interface Science and Engineering in Advanced Materials, Ministry of Education, 030024 Taiyuan, Shanxi Province, China; and Technology Center, Taiyuan Iron and Steel (Group) Company Limited, 030003 Taiyuan, China; and Technology Center, Taiyuan Iron and Steel (Group) Company Limited, 030003 Taiyuan, China
Min Ding*
Affiliation:
College of Materials Science and Engineering, Taiyuan University of Technology, 030024 Taiyuan, Shanxi Province, China; and Key Laboratory of Interface Science and Engineering in Advanced Materials, Ministry of Education, 030024 Taiyuan, Shanxi Province, China
*
a) Address all correspondence to this author. e-mail: [email protected]
Get access

Abstract

The effect of nitrogen gas addition in Ar-based double-layer shielding gas on the impact toughness of welded ultra-ferritic stainless steel during an autogenous gas tungsten arc welding (GTAW) process was investigated. The nitrogen behavior was proposed. The microstructure, mechanical properties, and fracture surface morphology of the weld metals have been evaluated. More equiaxed crystals, refined grain, narrow HAZ width, and increased microhardness were produced with nitrogen addition. Experimental findings indicated that nitrogen diffused into HAZ and dissolved into weld pool. The solute distribution was changed thus bringing significant constitutional supercooling and decreased temperature gradient of weld pool, which contributed to fine microstructure. Impact toughness at room temperature was enhanced from 2J to 9J (welds), 5J–13J (HAZ). Ductile fracture zone was produced about 0.3–0.5 mm thickness distance from the weld surface. A significant increased impact toughness of weld metal was due to the refinement of microstructure and element addition.

Type
Articles
Copyright
Copyright © Materials Research Society 2016 

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

REFERENCES

Wang, Y.C., Ding, M., Zheng, Y., Liu, S.S., Wang, W.X., and Zhang, Z.H.: Finite-element thermal analysis and grain growth behavior of HAZ on argon Tungsten-arc welding of 443 stainless steel. Met.-Open. Acc. Met. J. 6, 4 (2016).Google Scholar
Zheng, Y., Wang, Y.C., Li, H., Xing, W.Q., Yu, X.Y., Dong, P., Wang, W.X., Fan, G.W., Lian, J., and Ding, M.: An experimental study of nitrogen gas influence on the 443 ferritic stainless steel joints by double-shielded welding. Int. J. Adv. Manuf. Technol. (2016), doi: 10.1007/s00170-016-8693-2.Google Scholar
Amuda, M.O.H. and Mridha, S.: Comparative evaluation of grain refinement in AISI 430 FSS welds by elemental metal powder addition and cryogenic cooling. Mater. Des. 35, 609 (2012).CrossRefGoogle Scholar
Mallaiah, G., Reddy, P.R., and Kumar, A.: Influence of titanium addition on mechanical properties. Residual stresses and corrosion behaviour of AISI 430 grade ferritic stainless steel GTA welds. Proc. Mater. Sci. 6, 1740 (2014).Google Scholar
Watanabe, T., Shiroki, M., Yanagisawa, A., and Sasaki, T.: Improvement of mechanical properties of ferritic stainless steel weld metal by ultrasonic vibration. J. Mater. Process. Technol. 210, 1646 (2010).Google Scholar
Mallaiah, G., Kumar, A., Reddy, P.R., and Reddy, G.M.: Influence of grain refining elements on mechanical properties of AISI 430 ferritic stainless steel weldments—Taguchi approach. Mater. Des. 36, 443 (2012).Google Scholar
Amuda, M.O.H. and Mridha, S.: Grain refinement and hardness distribution in cryogenically cooled ferritic stainless steel welds. Mater. Des. 47, 365 (2013).CrossRefGoogle Scholar
Watanabe, Y., Takeda, T., and Sato, H.: Effect of magnetic field on weld zone by spotwelding in stainless steel. ISIJ Int. 46, 1292 (2006).CrossRefGoogle Scholar
Zhu, Z.X., Han, J., Li, H.J., and Lu, C.: High temperature processed high Nb X80 steel with excellent heat-affected zone toughness. Mater. Lett. 163, 171 (2016).Google Scholar
Li, J.Y., Chen, Y.L., and Huo, J.H.: Mechanism of improvement on strength and toughness of H13 die steel by nitrogen. Mater. Sci. Eng., A 640, 16 (2015).Google Scholar
Okagawa, R.K., Dixon, R.D., and Olson, D.L.: The influence of nitrogen from welding on stainless-steel weld metal microstructures. Weld. J. 62, S204 (1983).Google Scholar
Shi, Z.R., Wang, R.Z., Su, H., Chai, F., Wang, Q.F., and Yang, C.F.: Effect of nitrogen content on the second phase particles in V–Ti microalloyed shipbuilding steel during weld thermal cycling. Mater. Des. 96, 241 (2016).CrossRefGoogle Scholar
Bang, K.S., Chan, P., and Liu, S.: Effects of nitrogen content and weld cooling time on the simulated heat-affected zone toughness in a Ti-containing steel. J. Mater. Sci. 41, 5994 (2006).CrossRefGoogle Scholar
Lai, R., Cai, Y., Wu, Y., Li, F., and Hua, X.: Influence of absorbed nitrogen on microstructure and corrosion resistance of 2205 duplex stainless steel joint processed by fiber laser welding. J. Mater. Process. Technol. 231, 397 (2016).Google Scholar
Keskitalo, M., Mäntyjärvi, K., Sundqvist, J., Poweel, J., and Kaplan, A.F.H.: Laser welding of duplex stainless steel with nitrogen as shielding gas. J. Mater. Process. Technol. 216, 381 (2015).Google Scholar
Huang, H.Y.: Effects of shielding gas composition and activating flux on GTAW weldments. Mater. Des. 30, 2404 (2009).Google Scholar
Lin, Y.C. and Chen, P.Y.: Effect of nitrogen content and retained ferrite on the residual stress in austenitic stainless steel weldments. Mater. Sci. Eng., A 307, 165 (2001).Google Scholar
Shankar, V., Gill, T.P.S., Mannan, S.L., and Sundaresan, S.: Effect of nitrogen addition on microstructure and fusion zone cracking in type 316L stainless steel weld metals. Mater. Sci. Eng., A 343, 170 (2003).Google Scholar
Akhlaghi, M., Steiner, T., Meka, S.R., Leineweber, A., and Mittemeijer, E.J.: Lattice-parameter change induced by accommodation of precipitate/matrix misfit; misfitting nitrides in ferrite. Acta Mater. 98, 254 (2015).CrossRefGoogle Scholar
Fattahi, M., Nabhani, N., Vaezi, M.R., and Rahimi, E.: Improvement of impact toughness of AWS E6010 weld metal by adding TiO2, nanoparticles to the electrode coating. Mater. Sci. Eng., A 528, 8031 (2011).Google Scholar
Díaz-Fuentes, M., Iza-Mendia, A., and Gutiérrez, I.: Analysis of different acicular ferrite microstructures in low-carbon steels by electron backscattered diffraction. Study of their toughness behavior. Metall. Mater. Trans. A 34, 2505 (2003).Google Scholar
Li, X., Ma, X., Subramanian, S.V., Misra, R.D.K., and Shang, C.: Structure–property–fracture mechanism correlation in heat-affected zone of X100 ferrite−bainite pipeline steel. Metall. Mater. Trans. E 2, 1 (2015).Google Scholar
Kang, J., Li, C.N., Yuan, G., and Wang, G.D.: Improvement of strength and toughness for hot rolled low-carbon bainitic steel via grain refinement and crystallographic texture. Mater. Lett. 175, 157 (2016).Google Scholar
Kaijalainen, A.J., Suikkanen, P.P., Limnell, T.J., Karjalainen, L.P., Kömi, J.I., and Porter, D.A.: Effect of austenite grain structure on the strength and toughness of direct-quenched martensite. J. Alloy. Compd. 577, S642 (2013).Google Scholar