Hostname: page-component-586b7cd67f-gb8f7 Total loading time: 0 Render date: 2024-11-27T01:57:08.660Z Has data issue: false hasContentIssue false

Defect structure in single crystal titanium carbide

Published online by Cambridge University Press:  03 March 2011

Q.H. Zhao
Affiliation:
Department of Materials Science and Engineering, Oregon Graduate Inst. of Science and Technology, 20000 NW Walker Road, P.O. Box 91000, Portland, Oregon 97291–1000
J. Wu
Affiliation:
Department of Electrical Engineering and Applied Physics, Oregon Graduate Inst. of Science and Technology, 20000 NW Walker Road, P.O. Box 91000, Portland, Oregon 97291–1000
A.K. Chaddha
Affiliation:
Department of Electrical Engineering and Applied Physics, Oregon Graduate Inst. of Science and Technology, 20000 NW Walker Road, P.O. Box 91000, Portland, Oregon 97291–1000
H.S. Chen
Affiliation:
Department of Electrical Engineering and Applied Physics, Oregon Graduate Inst. of Science and Technology, 20000 NW Walker Road, P.O. Box 91000, Portland, Oregon 97291–1000
J.D. Parsons
Affiliation:
Department of Electrical Engineering and Applied Physics, Oregon Graduate Inst. of Science and Technology, 20000 NW Walker Road, P.O. Box 91000, Portland, Oregon 97291–1000
D. Downham
Affiliation:
Department of Materials Science and Engineering, Oregon Graduate Inst. of Science and Technology, 20000 NW Walker Road, P.O. Box 91000, Portland, Oregon 97291–1000
Get access

Abstract

The defects and crystallinity of as-grown and annealed TiCx (grown by the high-pressure float-zone) were examined by TEM and double crystal x-ray rocking curves. Three types of subboundaries and planar defects within subgrains were observed in as-grown TiCx. Subboundaries are classified by structure as (i) wide-extended, fault-like defects (WEFLD's), (ii) edge dislocation arrays, and (iii) dislocation networks. Planar defects were observed at dislocation nodes of subboundaries and also within subgrains; this is the first reported observation of planar defects within TiCx subgrains. The misorientation and/or density of subgrains in TiCx was reduced significantly by annealing at 2300 °C in contact with graphite.

Type
Articles
Copyright
Copyright © Materials Research Society 1994

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

REFERENCES

1Parsons, J. D., Bunshah, R. F., and Stafsudd, O. M., Solid State Technol., Nov., 133 (1985).Google Scholar
2Parsons, J. D., in Novel Refractory Semiconductors, edited by Emin, D., Aselage, T. L., and Wood, C. (Mater. Res. Soc. Symp. Proc. 97, Pittsburgh, PA, 1987), p. 271.Google Scholar
3Parsons, J. D., Kruaval, G. B., and Vigil, J. A., Amorphous and Crystalline Silicon Carbide and Related Materials II (Springer-Verlag, Berlin, Heidelberg, 1989), p. 171.Google Scholar
4Storms, E. K., The Refractory Carbides (Academic Press, New York, 1967), p. 8.Google Scholar
5Villars, P. and Calvent, L. D., Pearson's Handbook of Crystallographic Data for Intermetallic Phases (ASM, Metals Park, OH, 1985), Vol. 2, p. 1577.Google Scholar
6Chien, F. R., Nutt, S. R., and Cummings, D., Philos. Mag. A 68 (2), 325 (1993).Google Scholar
7Williams, W. S., Mater. Sci. Eng. A 105/106, 1 (1988).Google Scholar
8Williams, W. S. and Schaal, R. D., J. Appl. Phys. 33 (3), 955 (1962).Google Scholar
9Williams, W. S., J. Appl. Phys. 32, 552 (1961).CrossRefGoogle Scholar
10Hollox, G. E. and Smallman, R. E., J. Appl. Phys. 37 (3), 818 (1966).CrossRefGoogle Scholar
11Venable, J. D., Phys. Status Solidi 15, 413 (1966).Google Scholar
12Venable, J. D., Philos. Mag. 16, 873 (1967).Google Scholar
13Venable, J. D., Metall. Trans. 1, 2471 (1970).CrossRefGoogle Scholar
14Seegar, A., Dislocations and Mechanical Properties of Crystals (John Wiley, New York, 1957).Google Scholar
15Hirsch, P. B., Howie, A., Nicholson, R. B., and Pashley, D. W., Electron Microscopy of Thin Crystals (Butterworth, London, 1965).Google Scholar
16Edington, J. W., Practical Electron Microscopy (N.V. Phillips' Gloeilampenfabrieken, Eindhoven, The Netherlands, 1976).Google Scholar
17Friedel, J., Dislocations (Pergamon Press, New York, 1964), p. 275.Google Scholar
18Reed-Hill, R. E. and Abbaschian, R., Physical Metallurgy Principles, 3rd ed. (PWS-Kent Publishing Company, Boston, 1992), p. 227.Google Scholar
19Murr, L. E., Interfacial Phenomena in Metals and Alloys (Addison-Wesley Publishing Company, Reading, MA, 1975), p. 322.Google Scholar
20Smallman, R. E., Modern Physical Metallurgy (Butterworth, London, 1970), p. 387.Google Scholar
21Tiller, W. A., The Science of Crystallizations: Macroscopic Phenomena and Defects Generation (Cambridge University Press, 1991), p. 366.CrossRefGoogle Scholar
22Hirth, J. P. and Lothe, J., Theory of Dislocations (McGraw-Hill, Inc., New York, 1968), p. 672.Google Scholar