Apparatus for low-temperature growth of diamond-containing films

Published online by Cambridge University Press:  31 January 2011

P. H. Fang
Affiliation:
Department of Physics, Boston College, Chestnut Hill, Massachusetts 02167
J. H. Kinnier
Affiliation:
Department of Physics, Boston College, Chestnut Hill, Massachusetts 02167
Get access

Abstract

In current processes of diamond growth, the substrate temperature is in general around 600–900 °C. In the case of diamond-like carbon, the substrate temperature is lower, around 25–200 °C. There are many superior properties of diamond compared with diamond-like carbon; however, the high temperature requirement to grow diamond precludes many technologically important substrate materials such as zinc sulfide for an infrared window or electronic devices on which protective diamond layers are to be coated. The present approach is a hot filament DC glow discharge of hydrocarbon gases. A graphite hot filament cathode is inserted in a discharge cylinder tube anode. The discharge voltage is in the range of 50 to 250 volts at a methane gas pressure of about 100 microns. A negative biased voltage of 100 volts is applied between the cathode and the substrate. A magnetic field of 1 kG is applied near the cathode-anode assembly. At a substrate temperature of 200–400 °C, the deposited film on silicon crystal is confirmed by an electron diffraction pattern to consist of microcrystalline diamond.

Type
Articles
Copyright
Copyright © Materials Research Society 1989

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

REFERENCES

1Aksenov, I. I., Vakula, S. I., Padaika, V. G., Strelnitskii, V. E., and Khoroshikh, V. M., Sov. Phys. Tech. Phys. (Transl.) 25, 1164 (1980).Google Scholar
2Hiraki, A., Kawano, T., Kawakami, Y., and Miyasato, T., Solid State Commun. 50, 713 (1984).CrossRefGoogle Scholar
3Spitsyn, B. V. and Derjaguin, B. V., USSR Inv. Cert. No. 339134 (1956).Google Scholar
4Matsumoto, S., Sato, Y., Tsutsum, M., and Setaka, N., J. Mat. Sci. 17, 3106 (1982).CrossRefGoogle Scholar
5Namba, Y. and Mori, T., J. Vac. Sci. Tech. A3, 319 (1985).CrossRefGoogle Scholar
6Sawabe, A. and Inuzuka, T., Thin Solid Films 137, 89 (1986).CrossRefGoogle Scholar
7Suzuki, H., Matsubara, H., and Horie, N., J. Jpn. Soc. Powder Metallurgy 33, 281 (1986).CrossRefGoogle Scholar
8Shibuki, K. and Takatsu, S., Toshiba Tungaloy, Japan (private communication).Google Scholar
9This observation is made by Dr. Y. Sato.Google Scholar
10Inuzuka, T. and Sawabe, A., Appl. Phys. 55, 640 (1986) (in Japanese).Google Scholar