In a paper to the Faraday Society (1946), Mering showed that the temperature to which one required to heat montmorillonite to produce irreversible collapse of the c-axis depended on the exchangeable cation. With Na-montmorillonite irreversibility began at about 550°C but with Ca-montmorillonite below 350°C During a study of the liquid phase sorption of pyridine by montmorillonite, the writer obtained evidence that irreversible collapse occurred at 200°C with Li-montmorillonite.

The source of montmorillonite was a sample of Wyoming bentonite, which was purified by passing through a Sharples supercentrifuge. The resultant exchange capacity to ammonium acetate at pH 7 was about 90 m.e./100 gms. and the displaced ions chiefly consisted of Na+ and Ca++.

Type
Research Article
Copyright
Copyright © The Mineralogical Society of Great Britain and Ireland 1952

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

References

Mering, J. (1946). Trans. Faraday Soc., 42B, 205.Google Scholar
Gonzalez Garcia, F. (1950). Anales de Edafologia y Fisiologia Vegetal, 9, 149.Google Scholar
Hofmann, U. and Klemen, R. (1950). Z. Anorg. Chem., 262, 95.Google Scholar