Hostname: page-component-586b7cd67f-t7czq Total loading time: 0 Render date: 2024-11-27T03:53:03.331Z Has data issue: false hasContentIssue false

Oxidation of Zirconium-Yttrium Alloys

Published online by Cambridge University Press:  06 March 2019

D. I. Phalen
Affiliation:
Battelle Memorial Institute Columbus, Ohio
D. A. Vaughan
Affiliation:
Battelle Memorial Institute Columbus, Ohio
N. A. Richard
Affiliation:
Battelle Memorial Institute Columbus, Ohio
Get access

Abstract

The phase and elemental distributions on zirconium alloys containing 5, 10, 25, 35, and 50 at.%. yttrium, oxidized in dry air at 1200 and 1600°C, have been studied by X-ray diffraction, fluorescence, and electron-microprobe techniques. Zirconium-yttrium alloys, which are entirely solid at 1200°C, and zirconium 5 and 25 at.% yttrium alloys, which aire two-phase solid plus liquid at 1600°C, form a multiphase scale of ZrO2, Y2O3, and ZrN. The phase distribution varies with yttrium content, while the average metal composition remains constant throughout the oxide scale and base metal. In contrast, zirconium 35 and 50 at.% yttrium alloys, which are entirely liquid at 1600°C, form a single-phase Y2O3 layer.

The mechanism of air oxidation of solid zirconium-yttrium alloys, up to 50 at. % yttrium, is one of anion diffusion to the oxide-metal interface with little or no diffusion of the metallic elements. The oxidation of liquid alloys differs in that, as a result of yttrium diffusion to the oxide-liquid interface, Y2O3 is the only oxide formed. Ternary Zr-Y-O isotherms are presented to illustrate the phase distribution and mode of formation.

Type
Research Article
Copyright
Copyright © International Centre for Diffraction Data 1964

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

1. Didrinson, C. D. and Seigle, L. L., Experimental Study of Factors Controlling the Effectiveness of High-Temperature Protective Coatings for Tungsten, ASD-TDR-63-744, July 15, 1963.Google Scholar
2. Gschneidner, K. A. Jr., Rare Earth Alloys, D. Van Nostrand Company, Inc., Princeton, New Jersey, 1961.Google Scholar
3. Hansen, M. and Anderko, A., Constitution of Binary Alloys, second edition, McGraw-Hill Book Co., Inc., New York, 1958, p. 1078.Google Scholar
4. Love, B., Properties of Yttrium and the Rare Earth Metals, Oxygen, and Alloy Systems, WADD Technical Report 61-123, August, 1961.Google Scholar
5. Duwez, P., et al., “The Zirconia-Yttria System,” J. Electrochem, Soc. 98(9):356362, 1951.Google Scholar
6. Fu-Kang, F., et al., “Phase Relationships in the System YaOs-ZrOs: Part 2, Solid Solutions,” Bull. Akad. Sci. USSR, Div. Chem. Sa. (English Transi.) no. 4:542-549, April 1963.Google Scholar
7. Clark, J. B., “Conventions for Plotting the Diffusion Paths in Multiphase Ternary Diffusion Couples on the Isothermal Section of a Ternary Phase Diagram,” Trans. AIME 227:12501251, 1963.Google Scholar
8. Nicholas, M., et al, The Analysis of the Basic Factors Involved in the Protection of Tungsten Against Oxidation, Part I, ASD-TDR-62-20S, September 1962.Google Scholar