Abstract

In-situ corrosion tests on nuclear waste glasses in Boom clay provided direct contact glass-clay at 90°C, for periods of 2, 3.5 and 7.5 years. The corroded reference glasses (two R7T7 type glasses, four Pamela type glasses), were studied in terms of SIMS (secondary ion mass spectroscopy) and mass losses.

The Al2O3 rich Pamela glasses appear to corrode in a selective-substitutional way, the other glasses dissolve almost congruently. Differences in the corrosion extent between the glasses are associated with compositional differences and secondary phase formation. SIMS analysis provides the reaction layer thickness and the relative element behaviour in this layer. Although relatively few, the data have provided a coherent picture of glass corrosion, in terms of corrosion mechanisms, time and glass composition dependence.

Type
Research Article
Copyright
Copyright © Materials Research Society 1996

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

1. Iseghem, P.Van, in “Scientific Basis for Nuclear Waste Management XVII” Mat. Res. Soc. Proc. 333, 133 (1994)Google Scholar
2. Lodding, A., Ch. 4 in “Inorganic Mass Spectrometry” (F. Adams, R. Gijbels, R. van Grieken, Eds.), Wileys Chem. Analysis Series 95, NY (1988).Google Scholar
3. Lodding, A., Clark, D.E., Engström, E.U., Odelius, H., Schumacher, M., Zoitos, B.K., Wicks, G.G.., in “Ceramics Today -Tomorrow's Ceramics” (Vincenzini, P., Ed.), 3121–3129, Elsevier, Amsterdam (1991).Google Scholar
4. Lodding, A., Ch. 4 in “Corrosion of Glasses, Ceramics and Ceramic Superconductors” (Clark, D.E. & Zoitos, B.K., Eds.), Noyes Publ., Park Ridge, NJ (1992).Google Scholar
5. Lodding, A., Clark, D.E., Wicks, G.G., in “In-situ Testing of Radioactive Waste Forms and Engineered Barriers” (McMenamin, T., Ed.), EUR 15629-EN, in press. Preprint CEC (1993).Google Scholar
6. Wicks, G.G., Lodding, A., Macedo, P.B., Clark, D.E., in “Scientific Basis for Nuclear Waste Management XV”, Mat. Res. Soc. Proc. 257, 119 (1992).Google Scholar
7. Lodding, A., Iseghem, P.Van, in “In-situ Testing of Radioactive Waste Forms and Engineered Barriers” (McMenamin, T., Ed.), EUR 15629-EN, in press. Preprint CEC (1993).Google Scholar
8. Werme, L.O., Odelius, H., Lodding, A., in “In-situ Testing of Radioactive Waste Forms and Engineered Barriers” (McMenamin, T., Ed.), EUR 15629-EN, in press. Preprint CEC (1993).Google Scholar
9. Wicks, G.G., Lodding, A., Macedo, P.B., Clark, D.E., in “In-situ Testing of Radioactive Waste Forms and Engineered Barriers” (McMenamin, T., Ed.), EUR 15629-EN, in press. Preprint CEC (1993).Google Scholar
10. Iseghem, P.Van, Chen, H., in “In-situ Testing of Radioactive Waste Forms and Engineered Barriers” (McMenamin, T., Ed.), EUR 15629-EN, in press. Preprint CEC (1993).Google Scholar
11. Clark, D.E., Lodding, A., Odelius, H., Werme, L.O., Materials Sci. & Eng. 21, 241 (1987).Google Scholar
12. Iseghem, P.Van, Grambow, B., in “Scientific Basis for Nuclear Waste Management XI”, Mat. Res. Soc. Proc. 112, 631 (1988).Google Scholar