Application of Surface Photovoltage Spectroscopy in Surface Analysis

Published online by Cambridge University Press:  21 February 2011

Iain D. Baikie
Affiliation:
Department of Applied Physics, Robert Gordon's University, St. Andrew's Street, Aberdeen AB1 1HG, Scotland
Eimert Venderbosch
Affiliation:
Department of Applied Physics, University of Twente, 7500 AE Enschede, The Netherlands
Birgitta Hall
Affiliation:
Department of Physics, Linköping University, Linköping, Sweden
Get access

Abstract

Extension of the Kelvin probe vibrating capacitor technique of measuring work function, via Illumination of the semiconductor surface, i.e., Surface Photovoltage Spectroscopy (SPS), has many potential applications in the field of surface analysis.

The combination of broad-band (white) and monochromatic radiation, together with measurement of the dark signal permits complete characterisation of the semiconductor work function via determination of the electron-affinity, surface potential and Local DensIty-of-States (LDOS). The work function is an extremely sensitive indicator of a wide range of surface processes, e.g., particle adsorption, stress, defect creation, phase-transitions, etc.

We Illustrate application of this technique in the study of the temperature dependent initial oxidation behaviour of p-type Si(111) 7×7 between 100 and 300 K. The SPV response of the clean surface at 100 K corresponds to the capture of photo-stimulated electrons by a band of surface states centered around 1.4, 1.7, 1.9 and 2.4 eV. This response completely disappears at the peak of the (dark) work function change (0.3L) corresponding to a near complete removal of dangling bond states. The temperature-dependent white-light SPS response permits determination of the band-bending throughout the adsorption process. We observe that at 100 K the band-bending substantially decreases during the initial adsorption phase (0.1 L), after this dose it remains constant. However at 300 K the band-bending decreases much later, i.e., >10 L, in conjunction with oxygen permeation through the surface layer.

In conclusion Surface Photovoltage Spectroscopy SPS is a simple and flexible method which can be used to follow the rather complex changes occurring at the semiconductor surface. It is a non-contact, nondestructive technique which allows simultaneous determination of both semiconductor band-bending and electron affinity.

Type
Research Article
Copyright
Copyright © Materials Research Society 1992

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

REFERENCES

1. Thomson, W., later Lord Kelvin, Phil Nag. 46, 82 (1898).Google Scholar
2. Zisman, W.A., Rev. Scd. Instrum. 3, 267 (1932).Google Scholar
3. Baikie, I.D., Ph.D. Thesis, University of Twente, 1988.Google Scholar
4. Meyer, J.A., Balkie, I.D., Lopinski, G. P, Prybyla, J.A. and Estrup, P.J., J. Vac. Scl. Technol. A 8, 2468 (1990).Google Scholar
5. Kinlock, C. D and McMullen, A.I., J. Scl. Instrum. 36, 347 (1959).Google Scholar
6. Baikie, I.D., van der Werf, K.O., Oerbekke, H., Broeze, J. and van Silfhout, A., Rev.Sci.Instrum., 60, 930 (1989).Google Scholar
7. Balkle, I.D., van der Werf, K.O. and Hanekamp, L.J., Rev.Sci. Instrum., 59, 2075 (1988).Google Scholar
8. Anderson, P.A., Phys. Rev., 88, 655 (1952).Google Scholar
9. Baikie, I.D. In Chemical Perspectives of Microelectronic Materials, edited by Interrante, L.V., Jensen, K.F., Dubois, L.H. and Gross, H.E. (Mater. Res. Soc. Proc. 204, Pittsburgh, PA 1991, pp 363368.Google Scholar
10. Palau, J.M. and Bonnet, J., J. Phys. E. 21, 674 (1988).Google Scholar
11. Baikie, I.D., Mackenzie, S., Estrup, P.J.Z. and Meyer, J.A., Rev. Scl. Instrum., 62, 1326 (1991).CrossRefGoogle Scholar
12. Balkie, I.D., Venderbosch, E., Meyer, J.A. and Estrup, P.J.Z., Rev. Scl. Instrum 62, 725 (1991).Google Scholar
13. Silvestre, C. and Shayegan, M., Phys. Rev. B. 37, 10342 (1988).Google Scholar
14. Hofer, U., Wurth, W. and Umbach, E., Phys. Rev. B. 40, 1130 (1989).Google Scholar
15. Takayanai, K., Tanishiro, Y., Takahashi, M., Motoyoshi, H. and Yagl, K., J. Vac. Scl. Technol. A 3, 1502 (1985).Google Scholar
16. Law, J.T., J. Appl. Phys. 32, 600 (1961).Google Scholar
17. Avourls, P., J. Phys. Chem. 94, 2246 (1990).CrossRefGoogle Scholar
18. Avouris, P. and Wolkow, R.,Phys. Rev. B. 39, 5091 (1989).Google Scholar
19. Pelz, J.P. and Koch, R.H., Phys.Rev.B. 42,3761 (1990).Google Scholar