Hostname: page-component-5c6d5d7d68-wp2c8 Total loading time: 0 Render date: 2024-08-27T20:17:00.205Z Has data issue: false hasContentIssue false

Understanding of Inverse Coarsening of γ' precipitates in Ni-base Superalloys

Published online by Cambridge University Press:  25 July 2016

Subhashish Meher
Affiliation:
Materials Science and Engineering Department, Idaho National Laboratory, Idaho Falls, ID, 83415, USA
Larry K. Aagesen
Affiliation:
Fuels Modeling & Simulation Department, Idaho National Laboratory, Idaho Falls, ID, 83415, USA
Laura J. Carroll
Affiliation:
Materials Science and Engineering Department, Idaho National Laboratory, Idaho Falls, ID, 83415, USA
Mark C. Carroll
Affiliation:
Materials Science and Engineering Department, Idaho National Laboratory, Idaho Falls, ID, 83415, USA
Tresa M. Pollock
Affiliation:
Materials Department, University of California Santa Barbara, Santa Barbara, CA 93106, USA

Abstract

Image of the first page of this content. For PDF version, please use the ‘Save PDF’ preceeding this image.'
Type
Abstract
Copyright
© Microscopy Society of America 2016 

References

References:

[1] Su, C. H. & Voorhees, P. W. Acta Mater 44 (1996) 19871999.Google Scholar
[2] Johnson, W.C. Acta Metall 32 (1984) 465475.Google Scholar
[3] Sequeira, A. D., Calderon, H. A. & Kostorz, G. Scripta metall. mater 30 (1994) 712.Google Scholar
[4] Sequeira, A. D., Calderon, H. A., Kostorz, G. & Pedersen, J. S. Acta metall mater 43 (1995) 34413451.Google Scholar