No CrossRef data available.
Article contents
Model Materials for Irradiated Fuels: Study of Local Mechanical Behavior Using Nanoindentation and Microstructural Analysis
Published online by Cambridge University Press: 27 August 2014
Abstract
An abstract is not available for this content so a preview has been provided. As you have access to this content, a full PDF is available via the ‘Save PDF’ action button.
- Type
- Abstract
- Information
- Microscopy and Microanalysis , Volume 20 , Supplement S3: Proceedings of Microscopy & Microanalysis 2014 , August 2014 , pp. 1832 - 1833
- Copyright
- Copyright © Microscopy Society of America 2014
References
[2]
Dukino, R. D, et al. (1992), Journal of the American Ceramic Society, 75: 3299-3304.Google Scholar
You have
Access