In Situ Transmission Electron Microscopy Study on the Deformation Responses of Additively Manufactured Multiphase Ni-based Superalloy

Published online by Cambridge University Press:  30 July 2020

Qianying Guo
Affiliation:
Oak Ridge National Laboratory, Oak Ridge, Tennessee, United States
Michael M. Kirka
Affiliation:
Oak Ridge National Laboratory, Oak Ridge, Tennessee, United States
Kinga A. Unocic
Affiliation:
Oak Ridge National Laboratory, Oak Ridge, Tennessee, United States

Abstract

Image of the first page of this content. For PDF version, please use the ‘Save PDF’ preceeding this image.'
Type
In Situ TEM at the Extremes - Mechanical Behaviors
Copyright
Copyright © Microscopy Society of America 2020

References

Kaufman, M., Superalloys (1984), p. 43.Google Scholar
Mao, Z., et al. ., Acta Mat. 166 (2019), p. 702.10.1016/j.actamat.2019.01.017CrossRefGoogle Scholar
Sample was provided by the Manufacturing Demonstration Facility, which was sponsored by DOE's Office of Energy Efficiency and Renewable Energy. Microscopy conducted using instruments that are part of ORNL Nuclear Science User Facilities, which is a U.S. DOE Office of Science User Facility.Google Scholar