X-Ray Fractography on Fatigue Fractured Surface
Published online by Cambridge University Press: 06 March 2019
Extract
The technique analysing the cause and mechanism of fracture from the information obtained by X-ray irradiation on the fractured surface is called “X-ray fractography.” As a basic study of X-ray fractography the residual stress on the fatigue fractured surface and some parameters of the fracture mechanics were investigated.