Crossref Citations
This article has been cited by the following publications. This list is generated based on data provided by
Crossref.
Page, T. F.
Pharr, G. M.
Hay, J. C.
Oliver, W. C.
Lucas, B. N.
Herbert, E.
and
Riester, L.
1998.
Nanoindentation Characterisation of Coated Systems: P:S2 - A New Approach Using the Continuous Stiffness Technique.
MRS Proceedings,
Vol. 522,
Issue. ,
Hainsworth, S.V
McGurk, M.R
and
Page, T.F
1998.
The effect of coating cracking on the indentation response of thin hard-coated systems.
Surface and Coatings Technology,
Vol. 102,
Issue. 1-2,
p.
97.
Bull, S.J.
and
Korsunsky, A.M.
1998.
Mechanical properties of thin carbon overcoats.
Tribology International,
Vol. 31,
Issue. 9,
p.
547.
Strojny, Angela
Xinyun Xia
Tsou, Andy
and
Gerberich, William W.
1998.
Techniques and considerations for nanoindentation measurements of polymer thin film constitutive properties.
Journal of Adhesion Science and Technology,
Vol. 12,
Issue. 12,
p.
1299.
Bull, S.J.
and
Hainsworth, S.V.
1999.
Time-dependent changes in the mechanical properties of diamond-like carbon films.
Surface and Coatings Technology,
Vol. 122,
Issue. 2-3,
p.
225.
Malzbender, J.
and
de With, G.
2000.
The use of the loading curve to assess soft coatings.
Surface and Coatings Technology,
Vol. 127,
Issue. 2-3,
p.
265.
Malzbender, J.
and
de With, G.
2001.
The use of the indentation loading curve to detect fracture of coatings.
Surface and Coatings Technology,
Vol. 137,
Issue. 1,
p.
72.
Krupička, Andreas
Johansson, Mats
and
Hult, Anders
2003.
Viscoelasticity in Polymer Films on Rigid Substrates.
Macromolecular Materials and Engineering,
Vol. 288,
Issue. 2,
p.
108.
Hainsworth, S.V.
and
Soh, W.C.
2003.
The effect of the substrate on the mechanical properties of TiN coatings.
Surface and Coatings Technology,
Vol. 163-164,
Issue. ,
p.
515.
Berasategui, E.G.
and
Page, T.F.
2003.
The contact response of thin SiC-coated silicon systems—characterisation by nanoindentation.
Surface and Coatings Technology,
Vol. 163-164,
Issue. ,
p.
491.
Malzbender, Jürgen
2004.
Comment on ‘The concept of differential hardness in depth sensing indentation’.
New Journal of Physics,
Vol. 6,
Issue. ,
p.
C1.
Chowdhury, S.
Laugier, M.T.
and
Rahman, I.Z.
2004.
Measurement of the mechanical properties of carbon nitride thin films from the nanoindentation loading curve.
Diamond and Related Materials,
Vol. 13,
Issue. 4-8,
p.
1543.
Bull, S J
2005.
Nanoindentation of coatings.
Journal of Physics D: Applied Physics,
Vol. 38,
Issue. 24,
p.
R393.
Naimi-Jamal, M. R.
and
Kaupp, G.
2005.
Quantitative evaluation of nanoindents: Do we need more reliable mechanical parameters for the characterization of materials?.
Zeitschrift für Metallkunde,
Vol. 96,
Issue. 11,
p.
1226.
Ståhlberg, Daniel
Nordin, Lars‐Olof
Varna, Janis
and
Johansson, Mats
2005.
Mechanical Response of Thermoset Polymers under High Compressive Loads, 1.
Macromolecular Materials and Engineering,
Vol. 290,
Issue. 11,
p.
1063.
Korsunsky, Alexander M.
and
Constantinescu, Andrei
2006.
Work of indentation approach to the analysis of hardness and modulus of thin coatings.
Materials Science and Engineering: A,
Vol. 423,
Issue. 1-2,
p.
28.
Page, T. F.
and
Bull, S. J.
2006.
Measuring and modelling the instrumented indentation (nanoindentation) response of coated systems.
Philosophical Magazine,
Vol. 86,
Issue. 33-35,
p.
5331.
Hainsworth, S. V.
and
Uhure, N. J.
2007.
Diamond like carbon coatings for tribology: production techniques, characterisation methods and applications.
International Materials Reviews,
Vol. 52,
Issue. 3,
p.
153.
Roy, Marie E.
Whiteside, Leo A.
and
Katerberg, Brian J.
2009.
Diamond‐like carbon coatings enhance scratch resistance of bearing surfaces for use in joint arthroplasty: Hard substrates outperform soft.
Journal of Biomedical Materials Research Part B: Applied Biomaterials,
Vol. 89B,
Issue. 2,
p.
527.
Roy, M.E.
Whiteside, L.A.
Xu, J.
and
Katerberg, B.J.
2010.
Diamond-like carbon coatings enhance the hardness and resilience of bearing surfaces for use in joint arthroplasty.
Acta Biomaterialia,
Vol. 6,
Issue. 4,
p.
1619.