Abstract

The influence of film/electrolyte interface on structure and electrochromic properties of amorphous WO3 (a-WO3) films has been studied using cyclic voltammetry, optical electrochemistry and vibrational spectroscopy.

Type
Research Article
Copyright
Copyright © Materials Research Society 1997

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

REFERENCES

1. Deb, S.K., Sol. Ener. Mat. Sol. Cell, 25, 327 (1992).Google Scholar
2. Granquist, C.G., Thin SoUd Films, 193/194, 730 (1990).Google Scholar
3. Faughnan, B.W., Crandall, P.S., and Heyman, P.M., RCA Rev., 36, 177 (1975).Google Scholar
4. Shrimer, O.F., Wittwer, V., Baur, B., and Brandt, G., J. Electrochem. Soc, 124, 749 (1977).Google Scholar
5. Randin, J.P., J. Electron. Mat. 7, 47 (1978).Google Scholar
6. Gavrilko, T.A., Stepkin, V.I., and Shiyanovskaya, I.V., J. Mol. Struct., 218, 411 (1990).Google Scholar