Article contents
Synthesis of water dispersed Fe3O4@ZnO Composite Nanoparticles by the Polyol Method
Published online by Cambridge University Press: 13 July 2012
Abstract
Water-soluble Fe3O4@ZnO composite nanoparticles (NPs) were synthesized using a polyol route. The effects of the addition of the ZnO phase were evaluated by varying the Zn/Fe molar ratio in the 0.25-1.00 range as a function of the reaction time. X-ray diffractometry confirmed the formation of the magnetite and ZnO phases and suggested the possible formation of a composite structure. Also, using this method, pure magnetite and ZnO NPs were synthesized. The average crystallite sizes were estimated to 6.3 ± 0.3 nm and 8.6 ± 0.6 nm for magnetite and ZnO NPs, respectively. The samples were examined using transmission electron microscopy. Fourier transform infrared spectra indicated the presence of adsorbed species onto the solids surface, which may explain the good stability of the materials in water. Photoluminescence measurements at room temperature for pure ZnO nanoparticles exhibited the characteristic excitonic emission around 395 nm. Vibrating Sample Magnetometer measurements at room temperature evidenced the superparamagnetic behavior of magnetite nanocrystals, with a saturation magnetization of 60emu/g. The maximum magnetization ranged from 28 to 54emu/g for the composite NPs. Mössbauer spectroscopy measurements at room temperature showed evidence of evolving Fe-sites associated to superparamagnetic particles, as reflected on the coexistence of prominent doublet peaks and very weak sextet peaks.
- Type
- Articles
- Information
- Copyright
- Copyright © Materials Research Society 2012
References
- 2
- Cited by