Hostname: page-component-586b7cd67f-gb8f7 Total loading time: 0 Render date: 2024-11-25T18:23:33.604Z Has data issue: false hasContentIssue false

Properties of Glass Substrates for Poly-Si Amlcd Technology

Published online by Cambridge University Press:  15 February 2011

Dawne M. Moffatt*
Affiliation:
Corning Incorporated, Research and Development, SP-FR-5–1, Corning, New York 14831
Get access

Abstract

A major force for change in substrate requirements in the late 90's may well be the commercialization of poly-silicon thin film transistor (TFT) Active Matrix Liquid Crystal Display (AMLCDs) technology. The processes necessary for “poly-Si” occur at temperatures that are 150–300°C higher than the current amorphous-Si LCD processes. This impacts the thermal shrinkage and thermal gravimetric warp requirements of the glass, particularly as display resolutions tighten, as enabled by poly-Si. In addition, the expected integration of more components (e.g. chip-on-glass) impacts the requirements for the thermal expansion of the substrate.

One approach for meeting the poly-Si demands for greater thermal-dimensional stability is to use glasses with higher temperature capability. A new glass, Code 1737, with the highest strain point commercially available at over 660°C, now enables poly-Si processing with acceptable sag and shrinkage after annealing. A logical goal for the next significant glass advancement would be to eliminate annealing altogether, but it is unclear what temperature capability is required. In this study, various glasses with strain points ranging from 600–800°C have been evaluated in terms of their density, thermal expansion, and thermal shrinkage following poly-Si thermal process simulations. It has been confirmed that the magnitude of shrinkage decreases with increasing strain point for glasses in this compositional family. In addition, future new insight into the effect of thermal expansion coefficient has been developed; the lower the thermal expansion coefficient (for a given strain point), the lower the magnitude of the shrinkage for a given strain point and high temperature thermal cycle. This is important new learning in the area of substrates for flat panel displays that will help in further design and development of glasses for future AMLCDs.

Type
Research Article
Copyright
Copyright © Materials Research Society 1995

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

REFERENCES

1. Endo, Y., Masumo, K., Kunigita, M., Akatsuka, M. and Yuki, M., Conference Record of the 1991 International Display Research Conference, San Diego, October 1991, p. 203.Google Scholar
2. Wu, I.-W., Stuber, S., Tsai, C.C., Yao, W., Lewis, A., Chiang, A., and Thompson, M., SID 92 Digest, p. 615, May 1992.Google Scholar
3. Little, T. W., Koike, H., Takahara, K., Nakazawa, T., and Ohshima, H., Journal of the SID, 1[2] pp (1993).Google Scholar
4. Dumbaugh, W.H., SID 92 Digest, p. 805, May 1992.Google Scholar
5. Tool, A.Q., Journal of the Society of Glass Technology, 9, 185207 (1925).Google Scholar
6. Scherer, G. W., Relaxation in Glass and Composites, John Wiley and Sons (New York) 1986.Google Scholar
7. Buehl, W. M. and Ryszytiwskyj, W. P., SID Proceedings (1992).Google Scholar
8. Holbrook, D. S. and Donaher, J. C., SPIE Proceedings - Optical/Laser Microlithography IV, Volume 1463, March 1991.Google Scholar