Hostname: page-component-586b7cd67f-tf8b9 Total loading time: 0 Render date: 2024-11-29T08:04:17.222Z Has data issue: false hasContentIssue false

Annealing Behavior of the Hydrogen-Vacancy Complex in Bulk Indium Phosphide Crystals

Published online by Cambridge University Press:  10 February 2011

Q. Ye
Affiliation:
Materials Sciences Division, Lawrence Berkeley National Laboratory, Berkeley, CA 94720, [email protected]
J. A. Wolk
Affiliation:
Materials Sciences Division, Lawrence Berkeley National Laboratory, Berkeley, CA 94720, [email protected]
E. D. Bourret-Courchesne
Affiliation:
Materials Sciences Division, Lawrence Berkeley National Laboratory, Berkeley, CA 94720, [email protected]
D. F. Bliss
Affiliation:
United States Air Force Rome Laboratory, Hanscom Air Force Base, MA 01731
Get access

Abstract

In order to explain the effects of hydrogen on the electrical properties of bulk indium phosphide crystals, we have performed a series of high temperature annealing studies with both undoped and iron-doped indium phosphide crystals. Our samples were annealed at 900°C for 6, 36, and 72 hours, respectively, under a phosphorus overpressure of five atmospheres. Samples were characterized at 10 K by Fourier transform infrared absorption spectroscopy which allowed us to measure the concentrations of both the Fe2+ and VIn-H4 defects simultaneously. Undoped samples were further characterized by the Hall effect measurements. We find in the iron-doped samples that the [Fe2+]/[Fe3+] ratio decreases gradually with increasing annealing time, indicating a reduction in the number of donors in the samples. In the undoped samples, annealing leads to a reduction of the free electron concentration accompanied by an increase in the 77 K mobility. The increase of the sample's mobility eliminates the possibility that the reduction of the free electron concentration is due to an increase in the concentration of the compensating acceptors. Our explanation for the observed behavior in all samples is that hydrogen acts as a donor and it diffuses out of the crystal during the annealing process. Based on our experimental data, we propose a calibration equation of [VIn-H4] = 4.2×1016 cm−1 × Absorbance (cm−1) which is used to correlate the hydrogen-vacancy complex concentrations with the changes of the VIn-H4 absorption peak in both the iron-doped and the undoped samples. Our results confirm the donor nature of the hydrogen-vacancy complex and provide strong evidence regarding the reduction mechanism of free carrier concentrations in bulk indium phosphide crystals during high temperature annealing under a phosphorus atmosphere.

Type
Research Article
Copyright
Copyright © Materials Research Society 1998

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

REFERENCES

1. Kainosho, K., Shimakura, H., Yamamoto, H., and Oda, O., Appl. Phys. Lett., 59, 932 (1991).Google Scholar
2. Hofmann, D., Muller, G., and Steckful, N., Appl. Phys. A., 48, 315 (1989).Google Scholar
3. Kainosho, K., Ohta, M., Uchida, M., Nakamura, M., and Oda, O., J. Electr. Mat., 25, 353 (1996).Google Scholar
4. Zach, F. X., J. Appl. Phys., 75, 7894 (1994).Google Scholar
5. Zach, F. X., Bliss, D. F., Iseler, G. W., Walukiewicz, W., Bryant, G. G., Johnson, B., and Bourret-Courchesne, E. D., submitted to Phys. Rev. B.Google Scholar
6. Zach, F. X., Haller, E. E., Gabbe, D., Iseler, G. W., Bryant, G. G., and Bliss, D. F., J. Elec. Mater., 25, 331 (1996).Google Scholar
7. Alt, H. Ch., Treichler, R., and Volkl, J., Appl. Phys. Lett., 59, 3651 (1991).Google Scholar
8. Chevallier, J., Clerjaud, B., and Pajot, B., in Semiconductors and Semimetals, Volume 34, Academic Press, edited by Pankove, Jacques I. and Johnson, Noble M., Boston (1991).Google Scholar