Hostname: page-component-78c5997874-ndw9j Total loading time: 0 Render date: 2024-11-20T05:32:35.590Z Has data issue: false hasContentIssue false

Surface chemistry of Al(CH3)3 and TiCl4 on GaAs(100) and InGaAs during the first half-cycle of atomic layer deposition

Published online by Cambridge University Press:  23 November 2012

B. Granados
Affiliation:
Chemical and Environmental Engineering, University of Arizona, Tucson, AZ
F. Lie
Affiliation:
Chemical and Environmental Engineering, University of Arizona, Tucson, AZ
A. Muscat
Affiliation:
Chemical and Environmental Engineering, University of Arizona, Tucson, AZ
Get access

Abstract

Extended abstract of a paper presented at Microscopy and Microanalysis 2012 in Phoenix, Arizona, USA, July 29 – August 2, 2012.