Novel Characterization of Deformation Mechanisms in a Ni-base Superalloy Using HAADF Imaging and Atomic Ordering Analysis

Published online by Cambridge University Press:  25 July 2016

Donald McAllister
Affiliation:
The Ohio State University, Department of Materials Science and Engineering, Columbus, Ohio, USA
Duchao Lv
Affiliation:
The Ohio State University, Department of Materials Science and Engineering, Columbus, Ohio, USA
Hallee Deutchman
Affiliation:
Honeywell Aerospace, Phoenix, Arizona, USA
Benjamin Peterson
Affiliation:
Honeywell Aerospace, Phoenix, Arizona, USA
Yunzhi Wang
Affiliation:
The Ohio State University, Department of Materials Science and Engineering, Columbus, Ohio, USA
Michael J. Mills
Affiliation:
The Ohio State University, Department of Materials Science and Engineering, Columbus, Ohio, USA

Abstract

Image of the first page of this content. For PDF version, please use the ‘Save PDF’ preceeding this image.'
Type
Abstract
Copyright
© Microscopy Society of America 2016 

References

References:

[1] Sundararaman, M., et al., Acta Metall 36, 847864, 1988.CrossRefGoogle Scholar
[2] McAllister, D., et al., Scr. Mater 115, 108112, 2016.Google Scholar
[3] Phillips, P. J., et al., Appl. Phys. Lett 100, 211913 (2012).Google Scholar
[4] Geng, W., et al., Phys. Rev. B 76, 224102 (2007).CrossRefGoogle Scholar