Multi-Dimensional Machine Learning Aided Analysis of a Nickel-Based Superalloy

Published online by Cambridge University Press:  23 September 2015

David Rossouw
Affiliation:
Department of Materials Science and Metallurgy, University of Cambridge, 27 Charles Babbage Road, Cambridge, CB3 0FS, UK.
Robert Krakow
Affiliation:
Department of Materials Science and Metallurgy, University of Cambridge, 27 Charles Babbage Road, Cambridge, CB3 0FS, UK.
Zineb Saghi
Affiliation:
Department of Materials Science and Metallurgy, University of Cambridge, 27 Charles Babbage Road, Cambridge, CB3 0FS, UK.
Catriona S M Yeoh
Affiliation:
Department of Materials Science and Metallurgy, University of Cambridge, 27 Charles Babbage Road, Cambridge, CB3 0FS, UK.
Pierre Burdet
Affiliation:
Department of Materials Science and Metallurgy, University of Cambridge, 27 Charles Babbage Road, Cambridge, CB3 0FS, UK.
Rowan K Leary
Affiliation:
Department of Materials Science and Metallurgy, University of Cambridge, 27 Charles Babbage Road, Cambridge, CB3 0FS, UK.
Paul A Midgley
Affiliation:
Department of Materials Science and Metallurgy, University of Cambridge, 27 Charles Babbage Road, Cambridge, CB3 0FS, UK.

Abstract

Image of the first page of this content. For PDF version, please use the ‘Save PDF’ preceeding this image.'
Type
Abstract
Copyright
Copyright © Microscopy Society of America 2015 

References

References:

[1] Von Harrach, H. S., et al. J. Phys. Conf. Ser. 241 (2010). p. 012015.Google Scholar
[2] de la Pena, F., et al., Ultramicroscopy 111 (2011). p. 169.Google Scholar
[3] Burdet, P., et al., Acta Mater. 61 (2013). p. 3090.Google Scholar
[4] Midgley, P. A & Thomas, J. M., Angew. Chem. Int. Ed. Engl 53 (2014). p. 2.Google Scholar
[6] Viskari, L. & Stiller, K., Ultramicroscopy 111 (2011). p. 652.CrossRefGoogle Scholar
[7] Special thanks to Giorgio Divitini and Lech Staniewicz for preparation of the FIB prepared needle. D.R. acknowledges support from the Royal Society's Newton International Fellowship scheme..Google Scholar