Hostname: page-component-7bb8b95d7b-s9k8s Total loading time: 0 Render date: 2024-10-01T22:01:53.877Z Has data issue: false hasContentIssue false

Microstructure and Fractography of Eutectoid Fe30Ni20Mn35Al15

Published online by Cambridge University Press:  03 August 2008

Y Liao
Affiliation:
Dartmouth College
I Baker
Affiliation:
Dartmouth College
Get access

Extract

Extended abstract of a paper presented at Microscopy and Microanalysis 2008 in Albuquerque, New Mexico, USA, August 3 – August 7, 2008