Hostname: page-component-586b7cd67f-2plfb Total loading time: 0 Render date: 2024-11-26T09:33:25.604Z Has data issue: false hasContentIssue false

Investigation of failure mechanisms in ion irradiated X-750 Ni-based superalloy using transmission electron microscopy

Published online by Cambridge University Press:  30 July 2021

Zhongwen Yao
Affiliation:
Queen's University, Kingston, United States
Pooyan Changizian
Affiliation:
Queen's University, United States

Abstract

Image of the first page of this content. For PDF version, please use the ‘Save PDF’ preceeding this image.'
Type
Evaluation of Materials for Nuclear Applications
Copyright
Copyright © The Author(s), 2021. Published by Cambridge University Press on behalf of the Microscopy Society of America

References

Griffiths, M., "The Effect of Irradiation on Ni-containing Components in CANDU Reactor Cores: A Review", AECL Nuclear Review, Vol. 2, No. 1, 1-16, 2013.CrossRefGoogle Scholar
Changizian, P, Yao, Z, Daymond, MR, 'Deformation mechanism characteristics in a Ni-based alloy X-750: Dislocation/precipitate interaction' Materials Characterization 172, 110891, 2021.CrossRefGoogle Scholar