Effect of the Cooling Rate on the Microstructure Evolution of Haynes® 282® Ni-based Superalloy Subjected to γ′ Super-Solvus Heat Treatment

Published online by Cambridge University Press:  22 July 2022

A. Alexandratou*
Affiliation:
Lab. of Physical Metallurgy and Center for Electron Microscopy, School of Mining and Metallurgical Engineering, National Technical University of Athens, Heroon Polytechniou 9, 15780 Athens, Greece
S. Deligiannis
Affiliation:
Lab. of Physical Metallurgy and Center for Electron Microscopy, School of Mining and Metallurgical Engineering, National Technical University of Athens, Heroon Polytechniou 9, 15780 Athens, Greece
C. Roussos
Affiliation:
Lab. of Physical Metallurgy and Center for Electron Microscopy, School of Mining and Metallurgical Engineering, National Technical University of Athens, Heroon Polytechniou 9, 15780 Athens, Greece
N. I. Makris
Affiliation:
Lab. of Physical Metallurgy and Center for Electron Microscopy, School of Mining and Metallurgical Engineering, National Technical University of Athens, Heroon Polytechniou 9, 15780 Athens, Greece
A. Kaldellis
Affiliation:
Lab. of Physical Metallurgy and Center for Electron Microscopy, School of Mining and Metallurgical Engineering, National Technical University of Athens, Heroon Polytechniou 9, 15780 Athens, Greece
P. Tsakiridis
Affiliation:
Lab. of Physical Metallurgy and Center for Electron Microscopy, School of Mining and Metallurgical Engineering, National Technical University of Athens, Heroon Polytechniou 9, 15780 Athens, Greece
G. Fourlaris
Affiliation:
Lab. of Physical Metallurgy and Center for Electron Microscopy, School of Mining and Metallurgical Engineering, National Technical University of Athens, Heroon Polytechniou 9, 15780 Athens, Greece
*

Abstract

Image of the first page of this content. For PDF version, please use the ‘Save PDF’ preceeding this image.'
Type
General Physical Sciences
Copyright
Copyright © Microscopy Society of America 2022

References

Joseph, C., et al. , Philosophical Magazine Letters, 101:1 (2021), p. 30-39, doi: 10.1080/09500839.2020.1841314.CrossRefGoogle Scholar
Rakoczy, L., et al. , Materials 13(19):4452 (2020), doi: 10.3390/ma13194452.CrossRefGoogle Scholar
A. Alexandratou acknowledges the General Secretariat for Research and Technology (GSRT) and the Hellenic Foundation for Research and Innovation (HFRI) for the financial support.Google Scholar