Direct Observation of the SEI Layer Formation Process on the Graphite Anode by in situ TEM

Published online by Cambridge University Press:  22 July 2022

Weiqun Li
Affiliation:
Department of Mechanical, Materials and Aerospace Engineering, University of Liverpool, Liverpool, United Kingdom The Faraday Institution, Harwell Campus, Didcot, United Kingdom
Zachary Ruff
Affiliation:
Department of Chemistry, University of Cambridge, Cambridge, United Kingdom The Faraday Institution, Harwell Campus, Didcot, United Kingdom
Clare P. Grey
Affiliation:
Department of Chemistry, University of Cambridge, Cambridge, United Kingdom The Faraday Institution, Harwell Campus, Didcot, United Kingdom
B. Layla Mehdi*
Affiliation:
Department of Mechanical, Materials and Aerospace Engineering, University of Liverpool, Liverpool, United Kingdom Albert Crewe Centre for Electron Microscopy, University of Liverpool, Liverpool, United Kingdom The Faraday Institution, Harwell Campus, Didcot, United Kingdom
*
*Corresponding author: [email protected]

Abstract

Image of the first page of this content. For PDF version, please use the ‘Save PDF’ preceeding this image.'
Type
Insights into Phase Transitions in Functional Materials by In Situ/Operando TEM: Experiment Meets Theory
Copyright
Copyright © Microscopy Society of America 2022

References

Li, M et al. , Adv. Mater. 30 (2018), p. 1800561. doi: 10.1002/adma.201800561Google Scholar
Chae, S et al. , Angew. Chem., Int. Ed. 59 (2020), p. 110. doi: 10.1002/anie.201902085Google Scholar
Booth, SG et al. , APL Mater. 9 (2021), p. 109201. doi: 10.1063/5.0051092Google Scholar
Grey, CP and Hall, DS, Nat. Commun. 11 (2020), p. 6279. doi: 10.1038/s41467-020-19991-4CrossRefGoogle Scholar
Agubra, VA and Fergus, JW, J. Power Sources 268 (2014), p. 153. doi: 10.1016/j.jpowsour.2014.06.024CrossRefGoogle Scholar
An, SJ et al. , Carbon 105 (2016), p. 52. doi: 10.1016/j.carbon.2016.04.008Google Scholar
This work was supported by the EPSRC UK Faraday Institution under the Degradation (FIRG01) project.Google Scholar