Direct Observation of Single Atoms in Sinter-Resistant and Bimetallic Catalyst Systems Synthesized by Atomic Layer Deposition
Published online by Cambridge University Press: 09 October 2013
Abstract
Extended abstract of a paper presented at Microscopy and Microanalysis 2013 in Indianapolis, Indiana, USA, August 4 – August 8, 2013.