Designing and characterizing a complex concentrated gamma/gamma prime ‘superalloy’

Published online by Cambridge University Press:  25 July 2016

Bharat Gwalani
Affiliation:
Center for Advanced Research and Technology and Department of Materials Science and Engineering, University of North Texas, Denton, TX, USA
Vishal Soni
Affiliation:
Center for Advanced Research and Technology and Department of Materials Science and Engineering, University of North Texas, Denton, TX, USA
Talukder Alam
Affiliation:
Center for Advanced Research and Technology and Department of Materials Science and Engineering, University of North Texas, Denton, TX, USA
Raj Banerjee*
Affiliation:
Center for Advanced Research and Technology and Department of Materials Science and Engineering, University of North Texas, Denton, TX, USA
*
*Corresponding author: [email protected]

Abstract

Image of the first page of this content. For PDF version, please use the ‘Save PDF’ preceeding this image.'
Type
Abstract
Copyright
© Microscopy Society of America 2016 

References

References:

[1] Yeh, J-W., et al., Advanced Engineering Materials 6.5 (2004) 299303.Google Scholar
[2] Cantor, Brian Entropy 16.9 (2014) 47494768.Google Scholar
[3] Choudhuri, D., et al, Scripta Materialia 100 (2015) 3639.Google Scholar
[4] Xu, X. D., et al., Acta Materialia 84 (2015) 145152.Google Scholar