Analysis of Strain Localization at High Angle Grain Boundaries During Creep of a Polycrystalline Superalloy Using SEM-Based Digital Image Correlation

Published online by Cambridge University Press:  25 July 2016

C.E. Slone
Affiliation:
Center for Electron Microscopy and Analysis, The Ohio State University, Columbus, OH
M.J. Mills
Affiliation:
Center for Electron Microscopy and Analysis, The Ohio State University, Columbus, OH

Abstract

Image of the first page of this content. For PDF version, please use the ‘Save PDF’ preceeding this image.'
Type
Abstract
Copyright
© Microscopy Society of America 2016 

References

[1] Unocic, , et al., Materials Science and Engineering A 483–484 (2008) 2532.Google Scholar
[2] Walley, , et al., Experimental Mechanics 52 (2012) 405416.Google Scholar
[3] Bechetti, , et al., Metallurgical and Materials Transactions A 46 (2014) 739755.Google Scholar
[4] Carter, , et al., Materials Science & Engineering A 605 (2014) 127136.Google Scholar
[5] Kammers, , et al., Experimental Mechanics 53 (2013) 17431761.Google Scholar
[6] Stinville, , et al., Acta Materialia 98 (2015) 2942.Google Scholar
[7] This material is based upon work supported by the National Science Foundation Graduate Research Fellowship Program under Grant No. DGE-1343012. Any opinions, findings, and conclusions or recommendations expressed in this material are those of the authors and do not necessarily reflect the views of the National Science Foundation.Google Scholar