HRTEM and STEM HAADF Study of Microtwining During Creep Deformation in Nickel Based Superalloy Rene 104

Published online by Cambridge University Press:  05 August 2007

L Kovarik
Affiliation:
The Ohio State University
G Viswanathan
Affiliation:
The Ohio State University
R Unocic
Affiliation:
The Ohio State University
PM Sarosi
Affiliation:
The Ohio State University
M Mills
Affiliation:
The Ohio State University
Get access

Extract

Extended abstract of a paper presented at Microscopy and Microanalysis 2007 in Ft. Lauderdale, Florida, USA, August 5 – August 9, 2007