Interface control and design for SiC fiber-reinforced titanium aluminide composites

Published online by Cambridge University Press:  31 January 2011

Hsing-Pang Chiu
Affiliation:
Department of Materials Science and Engineering, University of California, Los Angeles, California 90024–1595
S.M. Jeng
Affiliation:
Department of Materials Science and Engineering, University of California, Los Angeles, California 90024–1595
J-M. Yang
Affiliation:
Department of Materials Science and Engineering, University of California, Los Angeles, California 90024–1595
Get access

Abstract

The effectiveness of several coating systems which were used as a diffusion barrier for the SiC fiber-reinforced titanium aluminide composites was investigated. TaC, TiC, TiB2, B, C/graded TiB2, and Ag/Ta were applied to the SiC fiber via chemical vapor deposition and physical vapor deposition. The interfacial compatibility, interfacial stability, thermal residual stress, interfacial bond strength, and the transverse fracture behavior of the composites with coated fibers were characterized and determined. The results show that none of the above coating systems can satisfy the requirements for a strong, tough, and damage-tolerant SiC fiber-reinforced titanium aluminide composite. Several multilayer, multifunctional coating systems are proposed.

Type
Articles
Copyright
Copyright © Materials Research Society 1993

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

REFERENCES

1Yang, J-M. and Jeng, S.M., J. Metals, Nov., 56 (1989).Google Scholar
2Clyne, T.W. and Watson, M.C., Comp. Sci. Technol. 42, 25 (1991).CrossRefGoogle Scholar
3Jeng, S. M., Yang, J-M., and Graves, J. A., J. Mater. Res. 8, 905 (1993).CrossRefGoogle Scholar
4Thaw, C. and Shatwell, B., in Titanium Aluminum Composites, edited by Smith, P. R., Balsone, S. J., and Nicholas, T., WL-TR–91–4020 (1991), p. 17.Google Scholar
5Lipsitt, H. L., in High-Temperature Ordered Intermetallic Alloys, edited by Koch, C. C., Liu, C. T., and Stoloff, N. S. (Mater. Res. Soc. Symp. Proc. 79, Pittsburgh, PA, 1985), p. 351.Google Scholar
6Kieschke, R.R., Somekh, R.E., and Clyne, T.W., Acta Metall. Mater. 39 (4), 427 (1991).Google Scholar
7Brindley, P.K., Bartolotta, P. A., and Klima, S.J., NASA TM–100956 (1988).Google Scholar
8Konitzer, D. G. and Loretto, M. H., Mater. Sci. Eng. A 107, 217 (1989).CrossRefGoogle Scholar
9Yang, D. M., Huang, C. X., Huang, D. T., and Zhao, X., in Controlled Interphases in Composite Materials, edited by Ishida, H. (Elsevier, New York, 1990), p. 199.CrossRefGoogle Scholar
10Steeds, J. W. and Rhodes, C. G., J. Am. Ceram. Soc. 68 (5), 136 (1985).Google Scholar
11Birks, N. and Meier, G.H., Introduction to High Temperature Oxidation of Metals (Edward Arnold, 1983).Google Scholar
12Ochiai, S. and Murakami, Y., J. Mater. Sci. 14, 831 (1979).Google Scholar
13Mikata, Y. and Taya, M., J. Comp. Mat. 19, 554 (1985).CrossRefGoogle Scholar
14Yang, J-M. and Jeng, S. M., JOM, June, 52 (1992).Google Scholar