X-ray fractography is a new method utilizing the X-ray diffraction technique to observe the fracture surface for the analysis of the micromechanisms and mechanics of fracture. X-ray residual stress has been confirmed to be a particularly useful parameter when studying the fracture surfaces of high strength steels. The method has been applied to the fracture surface of fracture toughness and fatigue specimens.