Waste Package Corrosion Studies Using Small Mockup Experiments

Published online by Cambridge University Press:  01 February 2011

B.E. Anderson
Affiliation:
Department of Geological Sciences, The University of Michigan, Ann Arbor, MI, USA
K.B. Helean
Affiliation:
Sandia National Laboratories, Albuquerque, NM, USA
C.R. Bryan
Affiliation:
Sandia National Laboratories, Albuquerque, NM, USA
P.V. Brady
Affiliation:
Sandia National Laboratories, Albuquerque, NM, USA
R.C. Ewing
Affiliation:
Department of Geological Sciences, The University of Michigan, Ann Arbor, MI, USA
Get access

Abstract

Understanding the corrosion of spent nuclear fuel (SNF) and the subsequent mobilization of released radionuclides, particularly under oxidizing conditions, is one of the key issues in evaluating the long-term performance of a nuclear waste repository. However, the large amounts of iron in the metal waste package may create locally reducing conditions that would lower corrosion rates for the SNF, as well as reduce the solubility of some key radionuclides, e.g., Tc and Np. In order to investigate the interactions among SNF-waste package-fluids, four smallscale (∼1:40 by length) waste package mockups were constructed using metals similar to those proposed for use in waste packages at the proposed repository at Yucca Mountain. Each mockup experiment differed with respect to water input, exposure to the atmosphere, and temperature. Simulated Yucca Mountain process water (YMPW) was injected into three of the mockups at a rate of 200 μL per day for five days a week using a calibrated needle syringe. The YMPW was prepared by equilibrating 50 mg/L silica as sodium metasilicate with air, and adding enough HCl to lower the pH to 7.6 in contact with an excess of powdered calcite.

X-ray powder diffraction and scanning electron microscopy confirm that, where corrosion occurred, the dominant corrosion product in all cases was magnetite. In the high temperature (60°C) experiment, hematite and a fibrous, Fe-O-Cl phase were also identified. The Fe(II)/Fe(III) ratios measured in the corrosion products using a wet chemistry technique indicate extremely low oxygen fugacities (10-36 bar). Experiments are in progress in which 0.1g powdered UO2 was included in the mock-up in order to investigate the relative kinetics of Fe and U oxidation and to identify the U corrosion products formed under these conditions.

Type
Research Article
Copyright
Copyright © Materials Research Society 2008

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

[1] O'Loughlin, E. J., Kelly, S. D., Cook, R. E., Csencsits, R., and Kemner, K. M., "Reduction of Uranium(VI) by Mixed Iron(II)/Iron(III) Hydroxide (Green Rust): Formation of UO2 Nanoparticles," Environmental Science and Technology, vol. 37, pp. 721727, 2003.Google Scholar
[2] Navratil, J. D., "Ion-Exchange Technology in Spent Fuel-Reprocessing," Journal of Nuclear Science and Technology, vol. 26, pp. 735743, 1989.Google Scholar
[3] ASTM, "Standard Specification for Chromium and Chromium-Nickel Stainless Steel Plate, Sheet, and Strip for Pressure Vessels and for General Applications," American Society for Testing and Materials, West Conshohocken, PN A 240/A 240M-02a, 2002.Google Scholar
[4] ASTM, "Standard Specification for High-Strength, Low-Alloy Structural Steel, up to 50ksi [345Mpa] Minimum Yield Point, with Atmospheric Corrosion Resistance," American Society for Testing and Materials, West Conshohocken, PN A 588/A588M-05, 2005.Google Scholar
[5] Langmuir, D. L., Aqueous environmental geochemistry. Upper Saddle River, NJ: Prentice-Hall, 1996.Google Scholar
[6] Harrar, J. E., Carley, J. F. et al. , "Report of the Committee to Review the Use of J-13 Well Water in Nevada Nuclear Waste Storage Investigations.," Lawrence Livermore National Laboratory, Livermore, California 1990.Google Scholar
[7] Domski, P. S., "In-package chemistry abstraction for wasteforms at Yucca Mountain, Rev 03B," BSC-DOE, Yucca Mtn. Project Office, Las Vegas, NV 2004.Google Scholar
[8] Stookey, L. L., "Ferrozine - a new spectrophotometric reagent for iron," Analytical Chemistry, vol. 42, pp. 779, 1970.Google Scholar
[9] Pratt, J. H., American Journal of Science, vol. 48, pp. 149, 1984.Google Scholar
[10] Husler, J. W., Anderson, B. E., Helean, K. B., Bryan, C. R., and Brady, P. V., "Ferrozine Micro-method for Determination of Iron in Solids," 2007.Google Scholar
[11] Pepper, S. E., Bunker, D. J., Bryan, N. D., Livens, F. R., Charnock, J. M., Pattrick, R. A. D., and Collison, D., "Treatment of radioactive wastes: An X-ray absorption spectroscopy study of the reaction of technetium with green rust," Journal of Colloid and Interface Science, vol. 268, pp. 408412, 2003.Google Scholar
[12] Janeczek, J. and Ewing, R. C., "Dissolution and alteration of uraninite under reducing conditions," Jounal of Nuclear Materials, vol. 190, pp. 157173, 1992.Google Scholar